| Line 260: | Line 260: | ||
*[http://labadviser.danchip.dtu.dk/images/c/ce/Litho_Tool_Package_-_3_Exposure_TARAN.pdf Slides on UV exposure] | *[http://labadviser.danchip.dtu.dk/images/c/ce/Litho_Tool_Package_-_3_Exposure_TARAN.pdf Slides on UV exposure] | ||
*[http://labmanager.dtu.dk/function.php?module=Machine&view=view&mach=339 Training Video: UV Mask Aligner]''' | *[http://labmanager.dtu.dk/function.php?module=Machine&view=view&mach=339 Training Video: UV Mask Aligner]''' | ||
*[http://podcast.llab.dtu.dk/ | *[http://podcast.llab.dtu.dk/fileadmin/podcasts/2016/DTUDanchip/1.053_Aligner_MA6_part1_operation-720p.mp4 Training Video: UV Mask Aligner Part I (Operation)] | ||
*[[Specific_Process_Knowledge/Lithography/UVExposure_Dose|Information on UV Exposure Dose]] | *[[Specific_Process_Knowledge/Lithography/UVExposure_Dose|Information on UV Exposure Dose]] | ||
*[http://labadviser.danchip.dtu.dk/index.php/Specific_Process_Knowledge/Lithography/UVExposure_Dose Information on UV Exposure Dose] | *[http://labadviser.danchip.dtu.dk/index.php/Specific_Process_Knowledge/Lithography/UVExposure_Dose Information on UV Exposure Dose] | ||
Revision as of 15:02, 29 February 2016

Feedback to this page: click here
Comparing lithography methods at DTU Danchip
| UV Lithography | DUV Stepper Lithography | E-beam Lithography | Nano Imprint Lithography | 2-Photon Polymerization Lithography | |
|---|---|---|---|---|---|
| Generel description | Pattern transfer via UltraViolet (UV) light | Pattern transfer via DeepUltraViolet (DUV) light | Patterning by electron beam | Pattern transfer via hot embossing(HE) | Direct writing via IR laser |
| Pattern size range |
|
|
|
|
|
| Resist type |
|
|
|
|
|
| Resist thickness range |
~0.5µm to 20µm |
~50nm to 2µm |
~30nm to 0.5 µm |
~ 100nm to 2µm |
droplet or coating |
| Typical exposure time |
2s-30s pr. wafer |
Process depended, depends on pattern, pattern area and dose |
Depends on dose, Q [µC/cm2], beam current, I [A], and pattern area, A [cm2]: t = Q*A/I |
Process depended, depends also on heating and cooling temperature rates |
Process depended, depends on pattern and dose |
| Substrate size |
|
|
We have cassettes that fit to
Only one cassette can be loaded at time |
|
|
| Allowed materials |
|
|
|
|
|
Equipment Pages
|
3D Lithography | ||
Knowledge and Information about Lithography
THIS SECTION IS UNDER CONSTRUCTION
|
Literature
|
UV Exposure
|
Development
|