DTU Nanolab has two EBL exposure systems, a JEOL JBX-9500FSZ and a Raith eLINE Plus system. The two systems are very different and new users should consult the EBL team to dertermine which system is appropriate for a particular project or type of sample. The general specifications of the two tools are given in the table below and may serve as a guideline for choice of system to use, especially the pros and cons list at the end of the table. | DTU Nanolab has two EBL exposure systems, a JEOL JBX-9500FSZ and a Raith eLINE Plus system. The two systems are very different and new users should consult the EBL team to dertermine which system is appropriate for a particular project or type of sample. The general specifications of the two tools are given in the table below and may serve as a guideline for choice of system to use, especially the pros and cons list at the end of the table. | ||
| Line 274: | Line 271: | ||
|- | |- | ||
|-style="background:LightGrey; color:black" | |-style="background:LightGrey; color:black" | ||
|''' | |'''mr EBL 6000.1''' | ||
|Negative | |Negative | ||
|[http://http://www.microresist.de/home_en.htm MicroResist] | |[http://http://www.microresist.de/home_en.htm MicroResist] | ||
| Line 299: | Line 296: | ||
| | | | ||
|[[media:Process Flow HSQ.docx|process flow HSQ]] | |[[media:Process Flow HSQ.docx|process flow HSQ]] | ||
[[/ | [[/Lithography/EBeamLithography/High resolution patterning with HSQ|High resolution patterning with HSQ]] | ||
|- | |- | ||
| Line 407: | Line 404: | ||
The process flow for a standard e-beam exposure on CSAR with Al on top can be found here [[media:Process Flow CSAR with Al.docx|Process Flow CSAR with Al]]. | The process flow for a standard e-beam exposure on CSAR with Al on top can be found here [[media:Process Flow CSAR with Al.docx|Process Flow CSAR with Al]]. | ||
= Literature on E-beam Lithography = | = Literature on E-beam Lithography = | ||
* Lithography, Wiley, 2011: Chapter 3, Electron Beam Lithography by Stefan Landis: http://onlinelibrary.wiley.com/doi/10.1002/9781118557662.ch3/summary | * Lithography, Wiley, 2011: Chapter 3, Electron Beam Lithography by Stefan Landis: http://onlinelibrary.wiley.com/doi/10.1002/9781118557662.ch3/summary | ||