Specific Process Knowledge/Thin film deposition/thermalevaporator: Difference between revisions
Appearance
| Line 51: | Line 51: | ||
*10Å - 1µm (Al) | *10Å - 1µm (Al) | ||
*10Å - 0.5µm (Ag) | *10Å - 0.5µm (Ag) | ||
*up to 100 nm (Cr | *up to 100 nm (Cr) | ||
*ask if in doubt or if you wish to exceed the limits | *ask if in doubt or if you wish to exceed the limits | ||
|- | |- | ||