Specific Process Knowledge/Lithography: Difference between revisions
m TPT udated, most links checked and updated |
No edit summary |
||
| Line 279: | Line 279: | ||
*Lithography TPT lecture videos: | *Lithography TPT lecture videos: | ||
**Current version (6 videos, 1:28 hours:minutes in total) on [https://www.youtube.com/playlist?list=PLjWVU97LayHCp7x9OujmVlZWLAnK4CDFR YouTube] | **Current version (6 videos, 1:28 hours:minutes in total) on [https://www.youtube.com/playlist?list=PLjWVU97LayHCp7x9OujmVlZWLAnK4CDFR YouTube] | ||
**Old version (7 videos, 2:41 hours in total) on [https://www.youtube.com/ | **Old version (7 videos, 2:41 hours in total) on [https://www.youtube.com/playlist?list=PLjWVU97LayHCHDueZ8qdT1LXJLGr4wLOa YouTube] | ||
*A full [https://www.youtube.com/watch?v=TdwUGOxCdUc&index=39&list=PLM2eE_hI4gSDjK4SiDbhpmpjw31Xyqfo_ lecture series] from a UT Austin course on microfabrication by "litho guru" Chris Mack. Half of the lectures are on (projection) lithography :-) | *A full [https://www.youtube.com/watch?v=TdwUGOxCdUc&index=39&list=PLM2eE_hI4gSDjK4SiDbhpmpjw31Xyqfo_ lecture series] from a UT Austin course on microfabrication by "litho guru" Chris Mack. Half of the lectures are on (projection) lithography :-) | ||
| Line 324: | Line 324: | ||
*[[Specific_Process_Knowledge/Lithography/Resist#UV_resist_comparison_table|UV resist process flows]] | *[[Specific_Process_Knowledge/Lithography/Resist#UV_resist_comparison_table|UV resist process flows]] | ||
*[[Specific_Process_Knowledge/Lithography/EBeamLithography#E-beam_resists_and_Process_flow|E-beam resist process flows]] | *[[Specific_Process_Knowledge/Lithography/EBeamLithography#E-beam_resists_and_Process_flow|E-beam resist process flows]] | ||
|} | |} | ||
<br clear="all" /> | <br clear="all" /> | ||
Revision as of 09:55, 7 February 2025
The content on this page, including all images and pictures, was created by DTU Nanolab staff, unless otherwise stated.
Feedback to this page: click here

There are four different types of lithography available at DTU Nanolab:
Comparing lithography methods at DTU Nanolab
| UV Lithography | DUV Stepper Lithography | E-beam Lithography | Nano Imprint Lithography | |
|---|---|---|---|---|
| Generel description | Pattern transfer via ultraviolet (UV) light | Pattern transfer via deep ultraviolet (DUV) light | Patterning by electron beam | Pattern transfer via hot embossing (HE) |
| Pattern size range |
~0.6 µm and up |
~200 nm and up |
~12 nm - 1 µm |
~20 nm and up |
| Resist type |
UV sensitive:
|
DUV sensitive
|
E-beam sensitive
|
Imprint polymers:
|
| Resist thickness range |
~0.5 µm to 200 µm |
~50 nm to 2 µm |
~30 nm to 1 µm |
~ 100 nm to 2 µm |
| Typical exposure time |
10 s - 3 min pr. wafer using mask aligners |
Process dependent:
Throughput is up to 60 wafers/hour |
Process dependent:
time [s] = Q*a/I |
Process dependent, including heating/cooling rates |
| Substrate size |
|
|
We have cassettes fitting:
Only one cassette can be loaded at a time |
|
| Allowed materials |
Any standard cleanroom material |
Any standard cleanroom material |
Any standard cleanroom material, except:
|
Any standard cleanroom material |
Equipment Pages
|
|
||
Lithography Tool Package Training
DTU Nanolab offers a Tool Package Training in Lithography (TPT Lithography). You are required to pass this course, in order to get access to the lithography equipment inside the DTU Nanolabs cleanroom facility. The course includes theory on lithographic processes and training videos for specific equipment. The theory part consists of lecture videos followed by quizzes for each section. Once that part has been completed successfully, you can begin the online training for the lithography equipment you need to use. After completing the online training, you can request hands-on training for the lithography equipment inside the cleanroom via training@nanolab.dtu.dk.
The course is available via DTU Learn. You sign up for the course by enrolling yourself in the course here.
Course Description
- Online lecture videos
- Quizzes for each section
- Equipment-related training videos
- Hands-on training
Hands on training can be requested via training@nanolab.dtu.dk.
Learning objectives
Learn about the fundamentals of lithography processing in a cleanroom fabrication lab:
- Coating
- Exposure
- Development
- Resist, substrates and pre-treatment
- Post-lithography steps
Knowledge and Information about Lithography