Specific Process Knowledge/Lithography/Strip: Difference between revisions
Appearance
| Line 132: | Line 132: | ||
{| class="wikitable" | {| class="wikitable" | ||
|- | |- | ||
! !! [[Specific_Process_Knowledge/Lithography/Strip#Plasma_Asher_4|Resist stripping]] !! [[Specific_Process_Knowledge/Lithography/Descum#Plasma_Asher_3:_Descum|Descum (PA3)]] !! [[Specific_Process_Knowledge/Lithography/Descum#Plasma_Asher_4|Descum (PA4&5)]] !! Surface treatment !! Other ashing of organic material | ! !! [[Specific_Process_Knowledge/Lithography/Strip#Plasma_Asher_4|Resist stripping]] !! [[Specific_Process_Knowledge/Lithography/Descum#Plasma_Asher_3:_Descum|Descum (PA3)]] !! [[Specific_Process_Knowledge/Lithography/Descum#Plasma_Asher_4|Descum (PA4 & 5)]] !! Surface treatment !! Other ashing of organic material | ||
|- | |- | ||
! scope=row style="text-align: left;" | Process pressure | ! scope=row style="text-align: left;" | Process pressure | ||