Jump to content

Specific Process Knowledge/Characterization/AFM: Atomic Force Microscopy: Difference between revisions

Bghe (talk | contribs)
Bghe (talk | contribs)
Line 5: Line 5:
=AFM Icon 1 & 2 =
=AFM Icon 1 & 2 =
[[Image:P6180008.JPG|right|thumb|300px| AFM Icon-Pt Positioned in clean room: C-1]]
[[Image:P6180008.JPG|right|thumb|300px| AFM Icon-Pt Positioned in clean room: C-1]]
[[Image:l.jpg|right|thumb|300px| AFM Icon-Pt 2 Positioned in the basement of building 346]]
[[Image:l.jpg|right|thumb|300px| AFM Icon-Pt 2 Positioned in the basement of building 346-904]]
DTU Nanolab has two pieces of Bruker AFM Dimension Icon-Pt. AFM stands for Atomic Force Microscope which is a scanning probe microscope where a sharp probe is scanned across a surface either in contact mode, tapping mode or PeakForce tapping mode. The outcome is a topographic plot of the surface. It has a lateral solution of about 1 nm and a vertical resolution of less than 1 Å which makes it very suitable for topographic characterization in the nanometer regime. The limiting factor however is often the size of the probe in use. The tip radius of curvature (ROC) can be from 2 nm up to more than 20 nm depending on the chosen probe. The half cone angle of the tip can vary from less than 3<sup>o</sup> to over 25<sup>o</sup> giving problems resolving high aspect ratio structures.  
DTU Nanolab has two pieces of Bruker AFM Dimension Icon-Pt. AFM stands for Atomic Force Microscope which is a scanning probe microscope where a sharp probe is scanned across a surface either in contact mode, tapping mode or PeakForce tapping mode. The outcome is a topographic plot of the surface. It has a lateral solution of about 1 nm and a vertical resolution of less than 1 Å which makes it very suitable for topographic characterization in the nanometer regime. The limiting factor however is often the size of the probe in use. The tip radius of curvature (ROC) can be from 2 nm up to more than 20 nm depending on the chosen probe. The half cone angle of the tip can vary from less than 3<sup>o</sup> to over 25<sup>o</sup> giving problems resolving high aspect ratio structures.