Specific Process Knowledge: Difference between revisions
Jump to navigation
Jump to search
2nd Level - Process Topic
The section below here is under construction
Line 670: | Line 670: | ||
|- | |- | ||
|} | |} | ||
==Overview of sample processing 5== | |||
{| {{Table}} | |||
|- valign="top" | |||
| | |||
{| class="wikitable collapsible collapsed" border="1" cellspacing="1" cellpadding="2" width="430px" | |||
! colspan="3" style="text-align:left;" | [[image:Clean your sample.png|x100px|Clean your sample]] Clean your sample | |||
|- | |||
!Entry page in LabAdviser | |||
!Techniques | |||
!Materials | |||
|- | |||
|[[Specific Process Knowledge/Wafer cleaning|Wafer cleaning]] | |||
|Soap Sonic | |||
|Removes dust and particles | |||
|- | |||
| | |||
|7-up & Piranha | |||
|Removes organics and alkali ions | |||
|- | |||
| | |||
|RCA | |||
|Two step process to remove organics and metals | |||
|- | |||
| | |||
|5% HF | |||
|Removes native oxide | |||
|- | |||
| | |||
|IMEC | |||
|Removing dust, organics and alkali ions and slightly polish the surface. | |||
Make the surface hydrophillic | |||
|- | |||
|} | |||
| | |||
{| class="collapsible wikitable collapsed" border="1" cellspacing="1" cellpadding="2" align="left" width="430px" | |||
!colspan="3" style="text-align:left;" | [[image:Dry your sample.png|x100px|Dry your sample]] Dry your sample | |||
|- | |||
!Entry page in LabAdviser | |||
!Techniques | |||
!Materials | |||
|- | |||
|[[Specific Process Knowledge/Wafer and sample drying|Wafer and sample drying]] | |||
|Spin dryers | |||
|Whole wafers | |||
|- | |||
| | |||
|Critial point dryer | |||
|Sensitive wafers | |||
|- | |||
|} | |||
| | |||
{| class="wikitable collapsible collapsed" border="1" cellspacing="1" cellpadding="2" align="left" width="430px" | |||
!colspan="3" style="text-align:left;" | [[image:Create a film on your sample.png|x100px|Create a layer/film on your sample]] Create a layer/film on your sample | |||
|- | |||
!Entry page in LabAdviser | |||
!Techniques | |||
!Materials | |||
|- | |||
|[[Specific Process Knowledge/Thermal Process/Oxidation| Thermal Process/Oxidation]] | |||
|Thermal oxidation | |||
|Thermal SiO2 | |||
|- | |||
|[[Specific Process Knowledge/Thin film deposition| Thin film deposition]] | |||
| | |||
| | |||
|- | |||
| | |||
|Sputter deposition | |||
|Si,SiO2,Si3N3,TiO2, metals | |||
|- | |||
| | |||
|Thermal evaporation | |||
|Al, ? | |||
|- | |||
| | |||
|E-beam evaporation | |||
|Metals | |||
|- | |||
| | |||
|LPCVD | |||
|Si3N4, SRN, SiO2, Si (poly and amorph) | |||
|- | |||
| | |||
|PECVD | |||
|Si3N4, SiO2, PBSG | |||
|- | |||
| | |||
|Electroplating | |||
|Ni | |||
|- | |||
| | |||
|Epitaxial growth /MOCVD | |||
|? | |||
|- | |||
|[[Specific Process Knowledge/Lithography/Coaters|Lithography/Coaters]] | |||
| | |||
| | |||
|- | |||
| | |||
|Spin coating | |||
|resists, polymers | |||
|- | |||
| | |||
|Spray coating | |||
|resists, polymers | |||
|- | |||
|} | |||
|- valign="top" | |||
| | |||
{| class="wikitable collapsible collapsed" border="1" cellspacing="1" cellpadding="2" align="left" width="430px" | |||
!colspan="3" style="text-align:left;" | [[image:Dope your sample.png|x100px|Dope your sample]] Dope your sample | |||
|- | |||
|- | |||
!Entry page in LabAdviser | |||
!Techniques | |||
!Materials | |||
|- | |||
|[[Specific Process Knowledge/Thin film deposition/PECVD| Thin film deposition/PECVD]] | |||
|PECVD | |||
|Deposition of SiO2 or Si3N4 doped with P,B and Ge | |||
|- | |||
|[[Specific Process Knowledge/Thin film deposition/Furnace LPCVD PolySilicon|Thin film deposition/Furnace LPCVD PolySilicon]] | |||
|LPCVD | |||
|Deposition of PolySi doped with B or P | |||
|- | |||
|[[Specific Process Knowledge/Thermal Process/Dope with Boron|Thermal Process/Dope with Boron]] | |||
|Predeposition and drive-in | |||
|Doping Silicon wafers with boron | |||
|- | |||
|[[Specific Process Knowledge/Thermal Process/Dope with Phosphorus|Thermal Process/Dope with Phosphorus]] | |||
|Predeposition and drive-in | |||
|Doping Silicon wafers with phosphorus | |||
|- | |||
|[[Specific Process Knowledge/Doping|Doping]] | |||
|Ion implant | |||
|? | |||
|- | |||
|} | |||
| | |||
{| class="wikitable collapsible collapsed" border="1" cellspacing="1" cellpadding="2" align="left" width="430px" | |||
!colspan="3" style="text-align:left;" | [[image:Thermal treat your sample.png|x100px|Thermal treatment of your sample]] Thermal treatment of your sample | |||
|- | |||
!Entry page in LabAdviser | |||
!Techniques | |||
!Materials | |||
|- | |||
|[[Specific Process Knowledge/Thermal Process|Thermal Process]] | |||
|Annealing | |||
|Si, PECVD layers | |||
|- | |||
| | |||
|Oxidation | |||
|Si wafers | |||
|- | |||
| | |||
|Doping with B/P | |||
|Si wafers | |||
|- | |||
| | |||
|Pyrolysis | |||
|Resists? | |||
|- | |||
|} | |||
| | |||
{| class="wikitable collapsible collapsed" border="1" cellspacing="1" cellpadding="2" align="left" width="430px" | |||
!colspan="3" style="text-align:left;" | [[image:Make a mask on your sample.png|x100px|Make a mask on your sample]] Make a mask on your sample | |||
|- | |||
!Entry page in LabAdviser | |||
!Techniques | |||
|- | |||
|[[Specific Process Knowledge/Lithography| Lithography]] | |||
| | |||
|- | |||
| | |||
|Photolithography | |||
|- | |||
| | |||
|Deep UV lithography | |||
|- | |||
| | |||
|E-beam lithography | |||
|- | |||
| | |||
|Imprinting | |||
|- | |||
|} | |||
|- valign="top" | |||
| | |||
{| class="wikitable collapsible collapsed" border="1" cellspacing="1" cellpadding="2" align="left" width="430px" | |||
!colspan="3" style="text-align:left;" | [[image:Transfer mask pattrn to your sample.png|x100px|Transfer mask pattern to your sample]] Transfer mask pattern to your sample | |||
|- | |||
!Entry page in LabAdviser | |||
!Techniques | |||
!Materials | |||
|- | |||
|[[Specific Process Knowledge/Etch| Etch]] | |||
| | |||
| | |||
|- | |||
| | |||
|Wet etch | |||
|Si, Glass, SiO2, Si3N4, Al, Cr, Ti, Au, Pt, InP, InGaAsP, GaAs/AlGaAs | |||
|- | |||
| | |||
|Dry etch | |||
|Any material | |||
|- | |||
|[[Specific Process Knowledge/Lithography/LiftOff| Lithography/Lift-off]] | |||
| | |||
|? | |||
|- | |||
|} | |||
| | |||
{| class="wikitable collapsible collapsed" border="1" cellspacing="1" cellpadding="2" align="left" width="430px" | |||
!colspan="3" style="text-align:left;" | [[image:Define your structure directly.png|x100px|Define the structure directly on your sample]] Define your structure directly | |||
|- | |||
!Entry page in LabAdviser | |||
!Techniques | |||
!Materials | |||
|- | |||
|[[Specific Process Knowledge/Imprinting|Imprinting]] | |||
|Imprinting | |||
|Polymers | |||
|- | |||
|[[Specific Process Knowledge/Direct Structure Definition|Direct Structure Definition]] | |||
|LASER machining | |||
| | |||
|- | |||
|[[Specific Process Knowledge/Lithography|Lithography]] | |||
|Lithographic definition | |||
|Resists | |||
|- | |||
|[[Specific Process Knowledge/Direct Structure Definition|Direct Structure Definition]] | |||
|Polymer Injection molding | |||
|Polymers | |||
|- | |||
|} | |||
| | |||
{| class="wikitable collapsible collapsed" border="1" cellspacing="1" cellpadding="2" align="left" width="430px" | |||
!colspan="3" style="text-align:left;" | [[image:Bond your samples together.png|x100px|Bond your samples together]] Bond your samples together | |||
|- | |||
!Entry page in LabAdviser | |||
!Techniques | |||
!Materials | |||
|- | |||
|[[Specific Process Knowledge/Bonding|Bonding]] | |||
|Eutectic bonding | |||
| | |||
|- | |||
| | |||
|Fusion bonding | |||
| | |||
|- | |||
| | |||
|Anodic bonding | |||
| | |||
|- | |||
|} | |||
|- valign="top" | |||
| | |||
{| class="wikitable collapsible collapsed" border="1" cellspacing="1" cellpadding="2" align="left" width="430px" | |||
!colspan="3" style="text-align:left;" | [[image:Characterize your sample.png|x100px|Characterize your sample]] Characterize your sample | |||
|- | |||
!Entry page in LabAdviser | |||
!What do you need to measure? | |||
!Technique/Method | |||
|- | |||
|[[Specific Process Knowledge/Characterization|Characterization]] | |||
|Sample Imaging, XY dimensions | |||
|Microscopy: optical,SEM,AFM | |||
|- | |||
| | |||
|Sample Topography | |||
|AFM,Profiling with stylus or optical | |||
|- | |||
| | |||
|Film thickness and optical constants | |||
|Ellipsometry,Reflectometry,Prism Coupling | |||
|- | |||
| | |||
|Film Stress | |||
|Profiling with stylus or optical | |||
|- | |||
| | |||
|Wafer thickness | |||
| | |||
|- | |||
| | |||
|Element analysis | |||
|XPS,EDX,SIMS | |||
|- | |||
| | |||
|Contact Angle | |||
| | |||
|- | |||
| | |||
|Resistivity | |||
|Four point probe | |||
|- | |||
| | |||
|Doping level/Carrier density | |||
| | |||
|- | |||
| | |||
|Photoluminescence | |||
| | |||
|- | |||
|} | |||
| | |||
{| class="wikitable collapsible collapsed" border="1" cellspacing="1" cellpadding="2" align="left" width="430px" | |||
!colspan="3" style="text-align:left;" | [[image:Pack your sample (back-end).png|x100px|Pack your sample (back-end)]] Pack your sample (back-end) | |||
|- | |||
!Entry page in LabAdviser | |||
!Techniques | |||
!Materials | |||
|- | |||
|[[Specific Process Knowledge/Back-end processing|Back-end processing]] | |||
|Chip/die mounting | |||
| | |||
|- | |||
| | |||
|Wire bonding | |||
| | |||
|- | |||
| | |||
|Dicing | |||
| | |||
|- | |||
|} | |||
| | |||
|- | |||
|} | |||
[[/temp| jmli test ]] | [[/temp| jmli test ]] |
Revision as of 13:14, 29 July 2014
Feedback to this page: click here
Choose the process topic you are interested in
The section below here is under construction ![Section under construction.jpg](/images/thumb/9/9a/Section_under_construction.jpg/70px-Section_under_construction.jpg)
Overview of sample processing 4
|
|
| |||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||
|
|
| |||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||
|
|
| |||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||
|
|
Overview of sample processing 5
|
|
| |||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||
|
|
| |||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||
|
|
| |||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||
|
|