Specific Process Knowledge/Lithography: Difference between revisions
Appearance
No edit summary |
No edit summary |
||
| Line 1: | Line 1: | ||
<!-- =<span style="background:#FF2800">THIS PAGE IS UNDER CONSTRUCTION</span>[[image:Under_construction.png|200px]]=--> | <!-- =<span style="background:#FF2800">THIS PAGE IS UNDER CONSTRUCTION</span>[[image:Under_construction.png|200px]]=--> | ||
[[Image:DUV_wafers.jpg| | [[Image:DUV_wafers.jpg|320x320px|right|frame|]] | ||
'''Feedback to this page''': '''[mailto:photolith@danchip.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.danchip.dtu.dk/index.php?title=Specific_Process_Knowledge/Lithography click here]''' | '''Feedback to this page''': '''[mailto:photolith@danchip.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.danchip.dtu.dk/index.php?title=Specific_Process_Knowledge/Lithography click here]''' | ||
Revision as of 12:24, 9 August 2013

Feedback to this page: click here
Comparing lithography methods at DTU Danchip
| UV Lithography | DUV Stepper Lithography | E-beam Lithography | Nano Imprint Lithography | 2-Photon Polymerization Lithography | |
|---|---|---|---|---|---|
| Generel description | Generel description - method 1 | Generel description - method 2 | Electron beam lithography | 4 | 5 |
| Pattern size range |
|
|
|
|
|
| Resist type |
|
|
|
|
|
| Resist thickness range |
|
|
|
|
|
| Typical exposure time |
2s-30s pr. wafer |
?-? pr. ? |
Depends on dose, Q [µC/cm2], beam current, I [A], and pattern area, A [cm2]: t = Q*A/I |
? pr. wafer |
? pr. µm2 |
| Substrate size |
|
|
We have cassettes that fit to
Only one cassette can be loaded at time |
|
|
| Allowed materials |
|
|
|
|
|