Specific Process Knowledge/Thin film deposition/thermalevaporator: Difference between revisions

Reet (talk | contribs)
Reet (talk | contribs)
No edit summary
 
(One intermediate revision by the same user not shown)
Line 1: Line 1:
'''Feedback to this page''': '''[mailto:labadviser@danchip.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.danchip.dtu.dk/index.php?title=Specific_Process_Knowledge/Thin_film_deposition/thermalevaporator click here]'''  
'''Feedback to this page''': '''[mailto:labadviser@nanolab.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.nanolab.dtu.dk/index.php?title=Specific_Process_Knowledge/Thin_film_deposition/thermalevaporator click here]'''  


<i> This page is written by <b>DTU Nanolab staff</b></i>
<i> This page is written by <b>DTU Nanolab staff</b></i>
Line 52: Line 52:
*10Å - 0.5µm (Ag)
*10Å - 0.5µm (Ag)
*up to 100 nm (Cr)
*up to 100 nm (Cr)
*ask if in doubt or if you wish to exceed the limits
*ask the [mailto:thinfilm@nanolab.dtu.dk Thin Film group] if in doubt or if you wish to exceed the limits
|-
|-
|style="background:LightGrey; color:black"|Deposition rate
|style="background:LightGrey; color:black"|Deposition rate