|style="background:LightGrey; color:black"|Coating thickness | |style="background:LightGrey; color:black"|Coating thickness | ||
|style="background:WhiteSmoke; color:black"| | |style="background:WhiteSmoke; color:black"| | ||
* AR-P 6200.09 (CSAR): | * AR-P 6200.09 (CSAR): 150-200 nm | ||
* AZ 5214E: 1.5-5 µm | * AZ 5214E: 1.5-5 µm | ||
* AZ MiR 701: 1.5-4 µm | * AZ MiR 701: 1.5-4 µm | ||