| Line 76: | Line 76: | ||
| 100% | | 100% | ||
| ?? mm/s | | ?? mm/s | ||
| [[nickel cutting green | | [[media:Nickel_shim_3_bursts_532nm%2C_F_255mm.doc|nickel cutting green parameters]] | ||
|- style="background:LightGray" valign="top" | |- style="background:LightGray" valign="top" | ||
| Mask making | | Mask making | ||