Specific Process Knowledge/Etch/III-V ICP/InP-InGaAsP-InGaAs: Difference between revisions
Appearance
| Line 118: | Line 118: | ||
|- | |- | ||
|Other tests made | |Other tests made | ||
|Comparing of this Cl2/H2 recipe with HBr recipe on e-beamed structures[[Media:HBr vs Cl2 InP etch comparison Aurimas.pptx]] ''(By Aurimas Sakana @photonic (nov 2019)) | |Comparing of this Cl2/H2 recipe with HBr recipe on e-beamed structures:[[Media:HBr vs Cl2 InP etch comparison Aurimas.pptx]] ''(By Aurimas Sakana @photonic (nov 2019)) | ||
'' | '' | ||