Specific Process Knowledge/Thermal Process/A4 Phosphor Pre-dep furnace: Difference between revisions
| Line 8: | Line 8: | ||
[[Image:A4.JPG|thumb|300x300px|Phosphorus Pre-dep furnace (A4). Positioned in cleanroom 2]] | [[Image:A4.JPG|thumb|300x300px|Phosphorus Pre-dep furnace (A4). Positioned in cleanroom 2]] | ||
The Phosphorus Pre-dep furnace (A4) is used to dope Si wafers with phosphorus to make conductive structures, etch stop layers etc. The doping source is phosphoryl chloride (commonly called phosphorus oxychloride) which is a colourless liquid with the formula POCl<sub>3</sub>. | The Phosphorus Pre-dep furnace (A4) is used to dope Si wafers with phosphorus to make conductive structures, etch stop layers etc. The doping source is phosphoryl chloride (commonly called phosphorus oxychloride) which is a colourless liquid with the chemical formula POCl<sub>3</sub>. | ||
A4 is the lowest furnace tube in the A-stack positioned in cleanroom B-1. The furnaces in the A-stack are the cleanest of all furnaces in the cleanroom. Be aware of that all wafers (including new wafers) have to be RCA cleaned before they enter the furnace, and please check the cross contamination information in LabManager before you use the furnace. | |||
'''The user manual, technical information and contact information can be found in LabManager:''' | '''The user manual, technical information and contact information can be found in LabManager:''' | ||
Revision as of 10:22, 1 April 2019
Feedback to this page: click here
Phosphorus Pre-dep furnace (A4)
The Phosphorus Pre-dep furnace (A4) is used to dope Si wafers with phosphorus to make conductive structures, etch stop layers etc. The doping source is phosphoryl chloride (commonly called phosphorus oxychloride) which is a colourless liquid with the chemical formula POCl3.
A4 is the lowest furnace tube in the A-stack positioned in cleanroom B-1. The furnaces in the A-stack are the cleanest of all furnaces in the cleanroom. Be aware of that all wafers (including new wafers) have to be RCA cleaned before they enter the furnace, and please check the cross contamination information in LabManager before you use the furnace.
The user manual, technical information and contact information can be found in LabManager:
Phosphorus Pre-dep furnace (A4)
Process knowledge
| Purpose |
|
|
|---|---|---|
| Process parameter range | Process Temperature |
|
| Process pressure |
| |
| Gasses on the system |
| |
| Substrates | Batch size |
|
| Substrate materials allowed |
|