==Coaters: Comparison Table==
{{cc-nanolab}}


{| border="2" cellspacing="0" cellpadding="2"
'''Feedback to this page''': '''[mailto:labadviser@nanolab.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.nanolab.dtu.dk/index.php?title=Specific_Process_Knowledge/Lithography/Coaters click here]'''


!colspan="2" border="none" style="background:silver; color:black;" align="center"|Equipment
[[Category: Equipment|Lithography coaters]]
|style="background:WhiteSmoke; color:black"|<b>SSE Spinner</b>
[[Category: Lithography|Coaters]]
|style="background:WhiteSmoke; color:black"|<b>KS Spinner</b>
 
|style="background:WhiteSmoke; color:black"|<b>Spin Track 1 + 2</b>
__TOC__
 
=Coater Comparison Table=
{| class="wikitable"
|-
!
! [[Specific_Process_Knowledge/Lithography/Coaters/GammaUV|Spin Coater: Gamma UV]]
! [[Specific_Process_Knowledge/Lithography/Coaters/GammaDUV|Spin Coater: Süss Stepper]]
! [[Specific_Process_Knowledge/Lithography/Coaters/GammaEbeam|Spin Coater: Gamma E-beam and UV]]
! [[Specific_Process_Knowledge/Lithography/Coaters/RCD8|Spin Coater: RCD8]]
! [[Specific_Process_Knowledge/Lithography/Coaters/labspin|Spin Coater: LabSpin 02]]
! [[Specific_Process_Knowledge/Lithography/Coaters/labspin|Spin Coater: LabSpin 03]]
! [[Specific_Process_Knowledge/Lithography/Coaters/labspin05|Spin Coater: LabSpin 05]]
! [[Specific_Process_Knowledge/Lithography/Coaters/sprayCoater|Spray Coater]]
|-
|-
!style="background:silver; color:black;" align="center"|Purpose  
! scope=row| Purpose  
|style="background:LightGrey; color:black"|  
|
|style="background:WhiteSmoke; color:black"|
*In-line substrate HMDS priming
*Spinning and baking of AZ5214E resist
*Coating and baking of  
*Spinning and baking of AZ4562 resist
**AZ MiR 701 (29cps)
*Spinning and baking of e-beam resist
**AZ nLOF 2020
|style="background:WhiteSmoke; color:black"|
**AZ 5214E
*Spinning and baking of AZ5214E resist
|
*Spinning and baking of AZ4562 resist
*Coating and baking of
*Spinning and baking of SU8 resist
**BARC (DUV42S-6)
|style="background:WhiteSmoke; color:black"|
**KRF M230Y
**KRF M35G
**UVN2300-0.8
|
*In-line substrate HMDS priming
*In-line substrate HMDS priming
*Coating and baking of AZ MiR 701 (29cps) resist
*Coating and baking of  
*Coating and baking of AZ nLOF 2020 resist
**AR-P 6200 (CSAR)
*Post-exposure baking at 110°C
**ZEP 520A diluted 1:2 (pay-per-use)
**AZ 5214E
**AZ MiR 701 (29cps)
**AZ 4562
*Edge bead removal on novolac-based resist and SU-8
|
*Coating of
**SU-8
**AZ 5214E
**AZ 4562
**AZ MiR
**AZ nLOF
*Edge bead removal
|colspan="2"|
*Coating of E-beam resists
** CSAR, ZEP, PMMA/MMA, HSQ(FOx)
*Coating of UV resists
**AZ5214E, AZ4562, AZMiR701, AZnLOF, SU-8
*Coating of imprint resists
|
*Coating of
**SU-8
**mr-DWL
**other resists
 
NB: this tool is in PolyFabLab
|
*Spraying imprint resist
*Spraying photoresist
*Spraying of other solutions
|-
|-
!style="background:silver; color:black" align="center" valign="center" rowspan="3"|Performance
! scope=row| Substrate handling
|style="background:LightGrey; color:black"|Substrate handling
|
|style="background:WhiteSmoke; color:black"|
* Cassette-to-cassette
* Cassette-to-cassette  
* Vacuum handling and detection
* Edge handling chuck
* Vacuum spin chuck
|style="background:WhiteSmoke; color:black"|
|
* Cassette-to-cassette
* Vacuum handling and detection
* Vacuum spin chuck
|
* Cassette-to-cassette
* Vacuum handling and detection
* Vacuum spin chuck
|
* Single substrate
* Vacuum chuck for 4" and 6"
* 4" non-vacuum chuck for fragile substrates
|colspan="2"|
* Single substrate
* Vacuum chucks for chips, 2", 4", and 6"
* 4" edge handling chuck
|
* Single substrate
* Single substrate
* Non-vacuum chuck for fragile substrates
* Vacuum chucks for chips, 4", and 6"
|style="background:WhiteSmoke; color:black"|
|style="background:WhiteSmoke; color:black"|
* Cassette-to-cassette
Can handle almost any sample size and shape
|-
|-
|style="background:LightGrey; color:black"|Permanent media
! scope=row| Permanent medias
|style="background:WhiteSmoke; color:black"|
|
* AZ5214E resist
* AZ4562 resist
* Acetone for chuck cleaning
* Acetone for drip pan
|style="background:WhiteSmoke; color:black"|
* AZ5214E resist
* PGMEA for edge bead removal
* Acetone for chuck cleaning
|style="background:WhiteSmoke; color:black"|
* AZ MiR 701 (29cps) resist
* AZ MiR 701 (29cps) resist
* AZ nLOF 2020 resist
* AZ nLOF 2020 resist
* PGMEA for backside rinse and edgebead removal
* AZ 5214E resist
* PGMEA for spinner bowl cleaning and vapor tip bath
* PGMEA solvent for backside rinse and spinner bowl cleaning
|
* DUV42S-6 (BARC)
* KRF M230Y resist
* KRF M35G resist
* PGMEA solvent for edge bead removal and backside rinse
|
* AR-P 6200.09 (CSAR) for 4", and 6"
* ZEP 520A diluted 1:2 for 4", and 6"
* AZ5214E for 4", and 6"
* AZ MiR 701 (29cps) for 4", and 6"
* AZ4562 for 4", and 6"
* PGMEA solvent for edge bead removal, backside rinse, and spinner bowl cleaning
|
No permanent media
|colspan="2"| Only manual dispense
| Only manual dispense
| No permanent media
|-
! scope=row| Manual dispense option
|
* No manual dispense
* Syringe dispense (60cc) of PGMEA-based resist
|
* No manual dispense
* Syringe dispense (60cc) of PGMEA and anisole-based resist
|
* No manual dispense
* Syringe dispense (30cc) of PGMEA and anisole-based resist (Coater1 only)
| Only manual dispense
|colspan="2"| Only manual dispense
| Only manual dispense
| Two syringe pumps
|-
|-
|style="background:LightGrey; color:black"|Manual dispense option
! scope=row| Spindle speed
|style="background:WhiteSmoke; color:black"|
| 10 - 6000 rpm
* 2 automatic syringes
| 10 - 6000 rpm
|style="background:WhiteSmoke; color:black"|
| 10 - 6000 rpm
* yes
| 10 - 5000 rpm (3000 rpm with non-vacuum chuck)
* pneumatic dispense for SU8 resist
|colspan="2"| 100 - 8000 rpm (3000 rpm with edge handling chuck)
|style="background:WhiteSmoke; color:black"|
| 100 - 8000 rpm
* no
| NA
|-
|-
!style="background:silver; color:black" align="center" valign="center" rowspan="2"|Process parameter range
! scope=row| Gyrset
|style="background:LightGrey; color:black"|Spindle speed
| No
|style="background:WhiteSmoke; color:black"|
| No
*Range
| No
|style="background:WhiteSmoke; color:black"|
| Optional (max. speed 3000 rpm)
*Range
|colspan="2"| No
|style="background:WhiteSmoke; color:black"|
| No
*10 - 9990 rpm
| NA
|-
|-
|style="background:LightGrey; color:black"|Parameter 2
! scope=row| Substrate size
|style="background:WhiteSmoke; color:black"|
|
*Range
*50 mm wafers (tool change required)
|style="background:WhiteSmoke; color:black"|
*100 mm wafers
*Range
*150 mm wafers
|style="background:WhiteSmoke; color:black"|
*200 mm wafers (tool change required)
*Range
|
*100 mm wafers
*150 mm wafers
*200 mm wafers (may require tool change)
|
*2" or 50 mm wafers (tool change required)
*100 mm wafers
*150 mm wafers
|
*100 mm wafer
*150 mm wafer
|colspan="2"|
*50 mm wafers
*100 mm wafers
*150 mm wafer
*small pieces down to 5x5 mm2
|
*100 mm wafers
*150 mm wafer
*small pieces down to 5x5 mm2
|
Any sample(s) that fit inside machine
|-
|-
!style="background:silver; color:black" align="center" valign="center" rowspan="3"|Substrates
! scope=row| Batch size
|style="background:LightGrey; color:black"|Batch size
| 1 - 25
|style="background:WhiteSmoke; color:black"|
| 1 - 25
*<nowiki>24</nowiki> 50 mm wafers
| 1 - 25
*<nowiki>24</nowiki> 100 mm wafers
| 1
*<nowiki>24</nowiki> 150 mm wafers
|colspan="2"| 1
|style="background:WhiteSmoke; color:black"|
| 1
*<nowiki>1</nowiki> 100 mm wafer
| 1
*<nowiki>1</nowiki> 150 mm wafer
|style="background:WhiteSmoke; color:black"|
*<nowiki>25</nowiki> 100 mm wafers
|-
|-
| style="background:LightGrey; color:black"|Allowed materials
! scope=row| Allowed substrate materials
|style="background:WhiteSmoke; color:black"|
|
*Allowed material 1
*Allowed material 2
|style="background:WhiteSmoke; color:black"|
*Allowed material 1
*Allowed material 2
*Allowed material 3
|style="background:WhiteSmoke; color:black"|
*Silicon  
*Silicon  
*Glass
*Glass
|-
|}


<br clear="all" />
'''No resist or crystalbond allowed in the HMDS module'''
|
*Silicon
*Glass
|
*Silicon
*III-V materials
*Glass


==SSE Spinner==
'''No resist or crystalbond allowed in the HMDS module'''
[[Image:SSEspinner2.jpg|200 × 200px|thumb|right|The SSE spinner MAXIMUS: positioned in Cleanroom 13.]]
|
All cleanroom materials except III-V materials
|colspan="2"|
*Silicon
*III-V materials
*Glass
|
All PolyFabLab materials
|
*All chemicals to be spray coated must be approved specifically for spray coating
*Any non-toxic, non-particulate and non-crosslinking material is likely to be approved
|-
|}


'''Feedback to this page''': '''[mailto:labadviser@danchip.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.danchip.dtu.dk/index.php/Specific_Process_Knowledge/Lithography/Coaters#SSE_Spinner click here]'''
=Spin coating=
The typical spin coating process consists of the following steps:
#Priming (typically HMDS) followed by cooling to room temperature
#Resist dispense (rotation: static or dynamic rotation)(arm: stationary or moving)
#*Optional: Acceleration to a low spin speed if dynamic dispense is used
#*Optional: Resist spreading at low spin speed for spreading thicker resists
#Spin-off
#Backside rinse (typically during spin-off)
#Optional: Edge-bead removal
#Softbake (contact or proximity)
#Cooling to room temperature


The SSE spinner MAXIMUS: positioned in Cleanroom 13.
SSE Spinner, Maximus 804, SSE Sister Semiconductor Equipment is a resist spinning system at Danchip which can be used for spinning on 2", 4" and 6" substrates.


The system is equipped with 2 different resists lines:
After priming, the wafer is cooled to room temperature and then transferred to the spin coater. If static dispense is used, the wafer is not rotating during the resist dispense. In the case of dynamic dispense, the wafer rotates at low spin speed during the dispense. The dispense arm is normally stationary during dispense, but some substrates may require the arm to move slowly across the substrate area while dispensing. Moving arm dispensing is usually only done with a rotating substrate.
*AZ5214E and  
*AZ4562 and
*2 syringe lines, which can be used for spinning of e-beam resist.  


The user manual(s), quality control procedure(s) and results and contact information can be found in LabManager: Equipment info in LabManager
Using too high spin speed during dispense can cause surface wetting issues, while a too low spin speed causes the resist to flow onto the backside of the wafer. After dispense, a short spin at low spin speed may be used in order to spread the resist over the wafer surface before spin-off.


A lot of text here.  A lot of text here.  A lot of text here.  A lot of text here.  A lot of text here.  A lot of text here. A lot of text here. A lot of text here. A lot of text here.  A lot of text here.  A lot of text here.  A lot of text here.  A lot of text here.  A lot of text here. A lot of text here. A lot of text here.
==Spin-off==
A lot of text here.  A lot of text here.  A lot of text here.  A lot of text here.  A lot of text here.  A lot of text here. A lot of text here. A lot of text here. A lot of text here.  A lot of text here.  A lot of text here.  A lot of text here. A lot of text here.  A lot of text here. A lot of text here. A lot of text here.
The spin-off cycle determines the thickness of the resist coating. For a given resist, the thickness is primarily a function of the spin-off speed and the spin-off time, both following an inverse power-law:


==Spin Track 1 + 2==
<math>y = k \sdot x^{-a}</math>


[[image:SpinTrack.jpg|300x257px|right|thumb|Spin Track 1 + 2 in Cleanroom 3]]
The acceleration to the spin-off speed also influences the thickness, but the effect is dependent on previous steps. The spin-off is usually a simple spin at one speed, but it may be comprised of several steps at different spin speeds. After spin-off, the wafer is decelerated.


'''Feedback to this page''': '''[mailto:labadviser@danchip.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.danchip.dtu.dk/index.php/Specific_Process_Knowledge/Lithography/Coaters#Spin_Track_1_.2B_2 click here]'''
The coated thickness, <math>t</math>, as a function of the spin-off speed, <math>w</math>, follows an inverse power-law:
<!-- Replace "http://labadviser.danchip.dtu.dk/..." wih the link to the Labadviser page-->


Spin Track 1 + 2 is an SVG 88 series track system from Rite Track. Each track consists of a HMDS priming module, a spin coating module, and a baking module. In fact, the only difference between the two tracks is the resist used in the spin coating module. Spin Track 1 + 2 is capable of handling 150 mm wafers, as well as 100 mm wafers, but is currently set up for 100 mm wafer processing.
<math>t=k \sdot w^{-a}</math>


The Spin Track 1 + 2 is controlled using the Recipe Manager software via the touchscreen on the arm attached to the lefthand end of the track. Recipes for the individual modules are developed by Danchip and combined into flows. The user selects a flow (specific to track 1 or 2), and the appropriate recipes will be downloaded and executed on the appropriate track. The other track runs an empty process (no wafers needed), and can unfortunately not be used by a second user while the first user is processing.
The constant, <math>k</math>, is a function of the resist viscosity and solid content, as well as the spin-off time. The exponent, <math>a</math>, is dependent on solvent evaporation, and is typically ~½ for UV resists. This means that from the thickness <math>t_1</math> achieved at spin speed <math>w_1</math>, one can estimate the spin speed <math>w_2</math> needed to achieve thickness <math>t_2</math> using the relation:


'''The user manual(s), quality control procedure(s) and results, user APV(s), technical information and contact information can be found in [http://labmanager.danchip.dtu.dk/function.php?module=Machine&view=view&mach=313 LabManager]'''
<math>t_1 \sdot w_1^{1/2} = t_2 \sdot w_2^{1/2} \rArr w_2 = w_1 \sdot \frac{t_1^2}{t_2^2}</math>
<!-- remember to remove the type of documents that are not present -->


===Process information===
[[Specific Process Knowledge/Lithography/Coaters/Spin Track 1 + 2 processing]]


[[Specific Process Knowledge/Lithography/Coaters/Spin Track 1 + 2/Spin Track 1 + 2 processing]]
For thick SU-8, however, <math>a</math> is observed to be ~1 (probably due to the low solvent content and/or the formation of skin). In this case, the relation simply becomes:


'''HMDS priming:'''
<math>t_1 \sdot w_1 = t_2 \sdot w_2 \rArr w_2 = w_1 \sdot \frac{t_1}{t_2}</math>


The process of HMDS priming on Spin Track 1 + 2 consists of five steps:
==Backside rinse==
*Contact bake
If the spin speed is too low during resist dispense, resist may creep over the edge of the wafer and onto the backside. Some resist tend to leave fine strings of resist protruding from the edge of the wafer, or folded onto the backside, an effect sometimes referred to as "cotton candy".  
*Vacuum bake
*Priming
*Pump-purge
*Cooling
The wafer is first baked in contact with the hotplate in order to heat the wafer to the hotplate temperature. The hotplates of the priming modules are set to 50°C. Then the wafer is baked under a low vacuum (~0.5 bar) in order to dehydrate the wafer before HMDS application. The HMDS is applied to the wafer using nitrogen as a carrier gas. 15 liters per minute of dry nitrogen is bubbled through liquid HMDS before flowing across the wafer surface. After the priming, the chamber is pump-purged twice, using a 7s pump to ~0.5 bar and a 10s nitrogen purge at 40 liters per minute. Finally, the wafer is cooled on the priming module coolplate.
 
The contact angle after HMDS priming is a function of the priming temperature, the priming time, and the surface condition of the wafer. Tests have shown the contact angle to decrease with increasing hotplate temperature, while it increases as a function of priming time at constant temperature. At a priming temperature of 50°C, the contact angle resulting from priming an oxidized silicon wafer for t = 30 - 300s may be approximated by
 
<math>\theta = 95 - 119.2 * t^{-0.51}</math>
 
The condition of the substrate surface is again a function of the substrate type, the substrate history, and the vacuum baking temperature and time. Since the vapor pressure of water at 50°C (0.123 bar) is lower than the vacuum bake pressure of 0.5 bar, the degree of dehydration will be a function of the vacuum baking time. Thus, for thick oxides, the standard of 30s vacuum bake may not be enough to dehydrate the surface sufficiently.
 
'''Spin coating:'''
 
Dispence. Spin-of. EBR. BSR.
 
'''Soft baking:'''
 
Contact or proximity. Bake. Cool.
 
'''Post-exposure baking:'''
 
Contact or proximity. Bake. Cool.
 
====HMDS priming only====
The standard HMDS priming process has been developed to mimic the behavior of the IMTEC Star2000 HMDS oven.
It produces a contact angle of 81-82° on an oxidized silicon surface.
 
''Flow names, process parameters, and test results:''
*T1 T2 HMDS Standard
Process: 10s contact bake, 30s vacuum bake, 72s HMDS priming, 5s cooling.
 
Tested 7/5 2013 on 110nm oxide: 81.4°. Tested 12/6 2013 on 3µm oxide: 81.8°. Tested 20/6 on 15µm oxide (dehydrated 1 hour at 250°C): 68-70°. Tested 21/6 on 15µm oxide (dehydrated 18 hours at 250°C): 71°.
 
====AZ MiR 701 (29cps) coating====
Spin coating of AZ MiR 701 (29cps) on Spin Track 1 is divided into two or three steps: HMDS priming (optional), spin coating, and soft baking. At the moment, the HMDS priming is equal to the standard priming, but this may be subject to change as our process knowledge grows. Spin coating uses dynamic dispence of 4 ml resist at 800 rpm, followed by spin-of at a thickness dependent spin speed for a thickness dependent time. The wafer is deaccelerated at 1000 rpm/s for 5 seconds before stopping. Soft baking is done at 90°C for 60s. As MiR 701 has a tendency to produce "cotton candy" on the edges, soft baking is performed in 1 mm proximity.
 
''Flow names, process parameters, and test results:''
*T1 MiR 701 1um no HMDS
*T1 MiR 701 1um with HMDS
Spin-of: 60 s at 9990 rpm.
 
Tested ?? (with HMDS) on fresh silicon: ? µm.
*T1 MiR 701 1,5um no HMDS
*T1 MiR 701 1,5um with HMDS
Spin-of: 30 s at 5000 rpm.
 
Tested 18/6 2013 (with HMDS) on fresh silicon: 1.5? µm.
*T1 MiR 701 2um no HMDS
*T1 MiR 701 2um with HMDS
Spin-of: 30 s at 2600 rpm.
 
Tested ?? (with HMDS) on fresh silicon: ? µm.
 
====AZ nLOF 2020 coating====
*T2 nLOF 2020 2um no HMDS
*T2 nLOF 2020 2um with HMDS
*T2 nLOF 2020 3um no HMDS
*T2 nLOF 2020 3um with HMDS
*T2 nLOF 2020 4um no HMDS
*T2 nLOF 2020 4um with HMDS
*T2 nLOF 2020 5um no HMDS
*T2 nLOF 2020 5um with HMDS
 
====Post-exposure baking====
*T2 5214E image reversal bake
*T2 MiR 701 PEB
*T2 nLOF 2020 PEB
 
Link to process pages - e.g. one page for each material
 
Example:
*[[Specific Process Knowledge/Etch/Etching of Silicon/Si etch using RIE1 or RIE2|Etch of silicon using RIE]]
*[[Specific Process Knowledge/Etch/Etching of Silicon Oxide/SiO2 etch using RIE1 or RIE2|Etch of silicon oxide using RIE]]
*[[Specific Process Knowledge/Etch/Etching of Silicon Nitride/Etch of Silicon Nitride using RIE|Etch of silicon nitride using RIE]]
*[[Specific Process Knowledge/Etch/Etching of Polymer/Etch of Photo Resist using RIE|Etch of photo resist using RIE]]
 
=== Equipment performance and process related parameters ===
 
{| border="2" cellspacing="0" cellpadding="2"
 
!colspan="2" border="none" style="background:silver; color:black;" align="center"|Spin Track
|style="background:WhiteSmoke; color:black" align="center"|<b>1</b>
|style="background:WhiteSmoke; color:black" align="center"|<b>2</b>
|-
!style="background:silver; color:black;" align="center" width="60"|Purpose
|style="background:LightGrey; color:black"|
|style="background:WhiteSmoke; color:black"|
*HMDS priming
*Spin coating and soft baking
*Priming, coating, and baking
|style="background:WhiteSmoke; color:black"|
*HMDS priming
*Spin coating and soft baking
*Priming, coating, and baking
*Post-exposure baking
|-
!style="background:silver; color:black;" align="center" width="60"|Resist
|style="background:LightGrey; color:black"|
|style="background:WhiteSmoke; color:black" align="center"|
AZ MiR 701 (29cps)
 
positive tone
|style="background:WhiteSmoke; color:black" align="center"|
AZ nLOF 2020
 
negative tone
|-
!style="background:silver; color:black" align="center" valign="center" rowspan="2"|Performance
|style="background:LightGrey; color:black"|Coating thickness
|style="background:WhiteSmoke; color:black" align="center"|
1 - 3 µm
|style="background:WhiteSmoke; color:black" align="center"|
1.6 - 5 µm
|-
|style="background:LightGrey; color:black"|HMDS contact angle
|style="background:WhiteSmoke; color:black" align="center" colspan="2"|
60 - 90° (on SiO2)
|-
!style="background:silver; color:black" align="center" valign="center" rowspan="4"|Process parameters
|style="background:LightGrey; color:black"|Spin speed
|style="background:WhiteSmoke; color:black" align="center" colspan="2"|
10 - 9990 rpm
|-
|style="background:LightGrey; color:black"|Spin acceleration
|style="background:WhiteSmoke; color:black" align="center" colspan="2"|
1000 - 50000 rpm/s
|-
|style="background:LightGrey; color:black"|Hotplate temperature
|style="background:WhiteSmoke; color:black" align="center"|
90°C
|style="background:WhiteSmoke; color:black" align="center"|
110°C
|-
|style="background:LightGrey; color:black"|HMDS priming temperature
|style="background:WhiteSmoke; color:black" align="center" colspan="2"|
50°C
|-
!style="background:silver; color:black" align="center" valign="center" rowspan="3"|Substrates
|style="background:LightGrey; color:black"|Substrate size
|style="background:WhiteSmoke; color:black" align="center" colspan="2"|
100 mm wafers
|-
| style="background:LightGrey; color:black"|Allowed materials
|style="background:WhiteSmoke; color:black" align="center" colspan="2"|
Silicon (with oxide, nitride, or metal films or patterning)
 
Glass (borosilicate and quartz)
|-
|style="background:LightGrey; color:black"|Batch
|style="background:WhiteSmoke; color:black" align="center" colspan="2"|
1 - 25
|-
|}


<br clear="all" />
Any resist on the edge and backside of the wafer will contaminate the end effector, softbake hotplate, and subsequent wafers.


==KS Spinner==
In a backside rinse step, solvent administered through a nozzle to the backside of the wafer, while spinning at low or medium spin speed, dissolves the resist and washes it away. After the rinse, a short spin at medium spin speed dries the wafer before the softbake.  
[[Image:KSspinner.JPG|200×200px|left|thumb|The KS spinner is placed in Cleanroom 3.]]


A lot of text here. A lot of text here. A lot of text here.  A lot of text here.  A lot of text here.  A lot of text here. A lot of text here. A lot of text here. A lot of text here.  A lot of text here.  A lot of text here.  A lot of text here.  A lot of text here.  A lot of text here. A lot of text here. A lot of text here.
During the backside rinse solvent inevitably creeps onto the front side of the wafer. This effect may be used to dissolve and subsequently remove an edge-bead, but it may also leave the rim of the wafer exposed. As an alternative to backside rinse, a wafer, which is contaminated on the backside, may be softbaked in proximity, in order to protect the hotplate from contamination. This leaves front side coating intact, but also leaves the backside dirty.
A lot of text here.  A lot of text here.  A lot of text here.  A lot of text here.  A lot of text here. A lot of text here. A lot of text here. A lot of text here. A lot of text here.  A lot of text here.  A lot of text here.  A lot of text here.  A lot of text here.  A lot of text here. A lot of text here. A lot of text here.


==Edge bead==
During spin coating, resist builds up at the edge of the wafer due to the change in surface tension at the edge, as well as extra drying from turbulence created by the wafer edge.


A lot of text here. A lot of text here. A lot of text here.  A lot of text here.  A lot of text here.  A lot of text here. A lot of text here. A lot of text here. A lot of text here.  A lot of text here.  A lot of text here.  A lot of text here.  A lot of text here.  A lot of text here. A lot of text here. A lot of text here.
This phenomenon is called edge-bead. Dependent on spin coating parameters, the coating may be several times thicker at the edge than in the central area. In a subsequent hard contact exposure step (mask aligner), this edge-bead introduces an undesired proximity gap, which reduces the lateral resolution, and may even cause the wafer to stick to the mask.  
A lot of text here.  A lot of text here.  A lot of text here.  A lot of text here.  A lot of text here.  A lot of text here. A lot of text here. A lot of text here. A lot of text here.  A lot of text here.  A lot of text here.  A lot of text here.  A lot of text here.  A lot of text here. A lot of text here. A lot of text here.


In an edge-bead removal step, solvent administered through a nozzle positioned at the edge of the wafer, while spinning at low or medium spin speed, dissolves the resist and washes it away. After the removal, a short spin at medium spin speed dries the wafer before the softbake. Dependent on the viscosity (solvent content) of the resist after the edge-bead removal, this drying spin may cause the resist to re-flow and create a secondary edge-bead. In some cases, it may be necessary to (partially) softbake the resist before edge-bead removal.


==Manual Spinner 1 (Laurell)==
==Softbake==
[[Image:Opticoat.jpg|200×200px|right|thumb|The Manual Spinner(Polymers) is placed in fumehood in Cleanroom 3.]]
After spin coating, the solvent in the resist must be evaporated in a baking step, in order to solidify the resist. This softbake can be carried out as a contact bake or a proximity bake. In a contact bake, the wafer is held in close contact to the hotplate surface, either in direct contact on the manual hotlpates or by resting on shallow bumps 150 µm above the hotplate in the Gamma tools. In a proximity bake, the wafer is first moved into proximity, e.g. 1mm, of the hotplate surface, then held there (on the lift pins) for the duration of the bake.


A lot of text here.  A lot of text here.  A lot of text here.  A lot of text here.  A lot of text here.  A lot of text here. A lot of text here. A lot of text here. A lot of text here.  A lot of text here.  A lot of text here.  A lot of text here.  A lot of text here.  A lot of text here. A lot of text here. A lot of text here.
=Decommisioned tools=
A lot of text here.  A lot of text here.  A lot of text here.  A lot of text here.  A lot of text here.  A lot of text here. A lot of text here. A lot of text here. A lot of text here.  A lot of text here.  A lot of text here.  A lot of text here.  A lot of text here.  A lot of text here. A lot of text here. A lot of text here.
<span style="color:red">The spin track was decommissioned 2018-02-01.</span>


A lot of text here.  A lot of text here.  A lot of text here.  A lot of text here.  A lot of text here.  A lot of text here. A lot of text here. A lot of text here. A lot of text here.  A lot of text here.  A lot of text here.  A lot of text here.  A lot of text here.  A lot of text here. A lot of text here. A lot of text here.
[[Specific Process Knowledge/Lithography/Coaters/Spin_Track_1_%2B_2_processing|Information about decommissioned tool can be found here.]]
A lot of text here.  A lot of text here.  A lot of text here.  A lot of text here.  A lot of text here.  A lot of text here. A lot of text here. A lot of text here. A lot of text here.  A lot of text here.  A lot of text here.  A lot of text here.  A lot of text here.  A lot of text here. A lot of text here. A lot of text here.

Latest revision as of 13:02, 15 September 2026

The content on this page, including all images and pictures, was created by DTU Nanolab staff, unless otherwise stated.

Feedback to this page: click here

Coater Comparison Table

Spin Coater: Gamma UV Spin Coater: Süss Stepper Spin Coater: Gamma E-beam and UV Spin Coater: RCD8 Spin Coater: LabSpin 02 Spin Coater: LabSpin 03 Spin Coater: LabSpin 05 Spray Coater
Purpose
  • In-line substrate HMDS priming
  • Coating and baking of
    • AZ MiR 701 (29cps)
    • AZ nLOF 2020
    • AZ 5214E
  • Coating and baking of
    • BARC (DUV42S-6)
    • KRF M230Y
    • KRF M35G
    • UVN2300-0.8
  • In-line substrate HMDS priming
  • Coating and baking of
    • AR-P 6200 (CSAR)
    • ZEP 520A diluted 1:2 (pay-per-use)
    • AZ 5214E
    • AZ MiR 701 (29cps)
    • AZ 4562
  • Edge bead removal on novolac-based resist and SU-8
  • Coating of
    • SU-8
    • AZ 5214E
    • AZ 4562
    • AZ MiR
    • AZ nLOF
  • Edge bead removal
  • Coating of E-beam resists
    • CSAR, ZEP, PMMA/MMA, HSQ(FOx)
  • Coating of UV resists
    • AZ5214E, AZ4562, AZMiR701, AZnLOF, SU-8
  • Coating of imprint resists
  • Coating of
    • SU-8
    • mr-DWL
    • other resists

NB: this tool is in PolyFabLab

  • Spraying imprint resist
  • Spraying photoresist
  • Spraying of other solutions
Substrate handling
  • Cassette-to-cassette
  • Vacuum handling and detection
  • Vacuum spin chuck
  • Cassette-to-cassette
  • Vacuum handling and detection
  • Vacuum spin chuck
  • Cassette-to-cassette
  • Vacuum handling and detection
  • Vacuum spin chuck
  • Single substrate
  • Vacuum chuck for 4" and 6"
  • 4" non-vacuum chuck for fragile substrates
  • Single substrate
  • Vacuum chucks for chips, 2", 4", and 6"
  • 4" edge handling chuck
  • Single substrate
  • Vacuum chucks for chips, 4", and 6"

Can handle almost any sample size and shape

Permanent medias
  • AZ MiR 701 (29cps) resist
  • AZ nLOF 2020 resist
  • AZ 5214E resist
  • PGMEA solvent for backside rinse and spinner bowl cleaning
  • DUV42S-6 (BARC)
  • KRF M230Y resist
  • KRF M35G resist
  • PGMEA solvent for edge bead removal and backside rinse
  • AR-P 6200.09 (CSAR) for 4", and 6"
  • ZEP 520A diluted 1:2 for 4", and 6"
  • AZ5214E for 4", and 6"
  • AZ MiR 701 (29cps) for 4", and 6"
  • AZ4562 for 4", and 6"
  • PGMEA solvent for edge bead removal, backside rinse, and spinner bowl cleaning

No permanent media

Only manual dispense Only manual dispense No permanent media
Manual dispense option
  • No manual dispense
  • Syringe dispense (60cc) of PGMEA-based resist
  • No manual dispense
  • Syringe dispense (60cc) of PGMEA and anisole-based resist
  • No manual dispense
  • Syringe dispense (30cc) of PGMEA and anisole-based resist (Coater1 only)
Only manual dispense Only manual dispense Only manual dispense Two syringe pumps
Spindle speed 10 - 6000 rpm 10 - 6000 rpm 10 - 6000 rpm 10 - 5000 rpm (3000 rpm with non-vacuum chuck) 100 - 8000 rpm (3000 rpm with edge handling chuck) 100 - 8000 rpm NA
Gyrset No No No Optional (max. speed 3000 rpm) No No NA
Substrate size
  • 50 mm wafers (tool change required)
  • 100 mm wafers
  • 150 mm wafers
  • 200 mm wafers (tool change required)
  • 100 mm wafers
  • 150 mm wafers
  • 200 mm wafers (may require tool change)
  • 2" or 50 mm wafers (tool change required)
  • 100 mm wafers
  • 150 mm wafers
  • 100 mm wafer
  • 150 mm wafer
  • 50 mm wafers
  • 100 mm wafers
  • 150 mm wafer
  • small pieces down to 5x5 mm2
  • 100 mm wafers
  • 150 mm wafer
  • small pieces down to 5x5 mm2

Any sample(s) that fit inside machine

Batch size 1 - 25 1 - 25 1 - 25 1 1 1 1
Allowed substrate materials
  • Silicon
  • Glass

No resist or crystalbond allowed in the HMDS module

  • Silicon
  • Glass
  • Silicon
  • III-V materials
  • Glass

No resist or crystalbond allowed in the HMDS module

All cleanroom materials except III-V materials

  • Silicon
  • III-V materials
  • Glass

All PolyFabLab materials

  • All chemicals to be spray coated must be approved specifically for spray coating
  • Any non-toxic, non-particulate and non-crosslinking material is likely to be approved

Spin coating

The typical spin coating process consists of the following steps:

  1. Priming (typically HMDS) followed by cooling to room temperature
  2. Resist dispense (rotation: static or dynamic rotation)(arm: stationary or moving)
    • Optional: Acceleration to a low spin speed if dynamic dispense is used
    • Optional: Resist spreading at low spin speed for spreading thicker resists
  3. Spin-off
  4. Backside rinse (typically during spin-off)
  5. Optional: Edge-bead removal
  6. Softbake (contact or proximity)
  7. Cooling to room temperature


After priming, the wafer is cooled to room temperature and then transferred to the spin coater. If static dispense is used, the wafer is not rotating during the resist dispense. In the case of dynamic dispense, the wafer rotates at low spin speed during the dispense. The dispense arm is normally stationary during dispense, but some substrates may require the arm to move slowly across the substrate area while dispensing. Moving arm dispensing is usually only done with a rotating substrate.

Using too high spin speed during dispense can cause surface wetting issues, while a too low spin speed causes the resist to flow onto the backside of the wafer. After dispense, a short spin at low spin speed may be used in order to spread the resist over the wafer surface before spin-off.

Spin-off

The spin-off cycle determines the thickness of the resist coating. For a given resist, the thickness is primarily a function of the spin-off speed and the spin-off time, both following an inverse power-law:

y=k⋅x−a

The acceleration to the spin-off speed also influences the thickness, but the effect is dependent on previous steps. The spin-off is usually a simple spin at one speed, but it may be comprised of several steps at different spin speeds. After spin-off, the wafer is decelerated.

The coated thickness, t, as a function of the spin-off speed, w, follows an inverse power-law:

t=k⋅w−a

The constant, k, is a function of the resist viscosity and solid content, as well as the spin-off time. The exponent, a, is dependent on solvent evaporation, and is typically ~½ for UV resists. This means that from the thickness t1 achieved at spin speed w1, one can estimate the spin speed w2 needed to achieve thickness t2 using the relation:

t1⋅w11/2=t2⋅w21/2⇒w2=w1⋅t12t22


For thick SU-8, however, a is observed to be ~1 (probably due to the low solvent content and/or the formation of skin). In this case, the relation simply becomes:

t1⋅w1=t2⋅w2⇒w2=w1⋅t1t2

Backside rinse

If the spin speed is too low during resist dispense, resist may creep over the edge of the wafer and onto the backside. Some resist tend to leave fine strings of resist protruding from the edge of the wafer, or folded onto the backside, an effect sometimes referred to as "cotton candy".

Any resist on the edge and backside of the wafer will contaminate the end effector, softbake hotplate, and subsequent wafers.

In a backside rinse step, solvent administered through a nozzle to the backside of the wafer, while spinning at low or medium spin speed, dissolves the resist and washes it away. After the rinse, a short spin at medium spin speed dries the wafer before the softbake.

During the backside rinse solvent inevitably creeps onto the front side of the wafer. This effect may be used to dissolve and subsequently remove an edge-bead, but it may also leave the rim of the wafer exposed. As an alternative to backside rinse, a wafer, which is contaminated on the backside, may be softbaked in proximity, in order to protect the hotplate from contamination. This leaves front side coating intact, but also leaves the backside dirty.

Edge bead

During spin coating, resist builds up at the edge of the wafer due to the change in surface tension at the edge, as well as extra drying from turbulence created by the wafer edge.

This phenomenon is called edge-bead. Dependent on spin coating parameters, the coating may be several times thicker at the edge than in the central area. In a subsequent hard contact exposure step (mask aligner), this edge-bead introduces an undesired proximity gap, which reduces the lateral resolution, and may even cause the wafer to stick to the mask.

In an edge-bead removal step, solvent administered through a nozzle positioned at the edge of the wafer, while spinning at low or medium spin speed, dissolves the resist and washes it away. After the removal, a short spin at medium spin speed dries the wafer before the softbake. Dependent on the viscosity (solvent content) of the resist after the edge-bead removal, this drying spin may cause the resist to re-flow and create a secondary edge-bead. In some cases, it may be necessary to (partially) softbake the resist before edge-bead removal.

Softbake

After spin coating, the solvent in the resist must be evaporated in a baking step, in order to solidify the resist. This softbake can be carried out as a contact bake or a proximity bake. In a contact bake, the wafer is held in close contact to the hotplate surface, either in direct contact on the manual hotlpates or by resting on shallow bumps 150 µm above the hotplate in the Gamma tools. In a proximity bake, the wafer is first moved into proximity, e.g. 1mm, of the hotplate surface, then held there (on the lift pins) for the duration of the bake.

Decommisioned tools

The spin track was decommissioned 2018-02-01.

Information about decommissioned tool can be found here.