Specific Process Knowledge/Lithography/Descum
Feedback to this page: click here
Descum results
Plasma asher 1
Descum of AZ5214E resist on 50mm silicon wafer. Wafer was placed horisontally in chamber on a 100 mm carier wafer.
Note: Plasma asher was cold before use
| ||||||||||||||||||||||||||||||||||||||||||||||||||
Conny Hjort & Jesper Hanberg September 2019
Descum of different resists, AZ5214E, AZ701 MiR and AZ2020 nLOF, on a single 100mm wafer was tested. Wafer was placed vertically in the middle of glass carrier. Recipe setting was the same as in previous test in September 2019: 70ml/min O2, 70 ml/min N2, power 150W, different ashing time 1, 2, 3, 5 and 7 min run. Plasma Asher was cold before use, we observed minor temperature rise during processing, but not more than 5 degrees. Starting chambers pressure was around 0, 5 mbar.
Plasma asher 2
Descum of AZ Mir 701 resist on 100mm silicon wafer. Five wafers were placed vertically in chamber.
Experiment parameters:
|
recipe 1
|
recipe 2
|
We can observe linear dependance of etched material on time after etching 7 minutes and more (recipe 2).
Jitka Urbánková & Jesper Hanberg
December 2019