Die bonder (eutectic metal soldering)

The Cammax EDB80 Die bonder is for placing and soldering dies onto a package or substrate.

The user manual(s), quality control procedure(s) and results, user APV(s), technical information and contact information can be found in LabManager:

File:Cluster1.jpg
Image(s) of the equipment(s)

Die Bonder in LabManager

Process information

Equipment performance and process related parameters

Equipment Die bonder Flip-chip bonder
Purpose
  • Fine placement of dies
  • Eutectic metal soldering
  • Fine placement of dies
  • glue attachment
Performance
  • Low thermal resistance
  • Always conducting
  • Medium or High thermal resistance
  • Possibility of both conducting and isolating adhesives
  • If an epoxy based adhesive is used the user is required to have the epoxy course.
Substrates Allowed materials
  • Should be able to withstand the soldering temperature
  • Typical materials are: Alumina (Al2O3), AluminumNitride (AlN)
  • Any that is compatible with the glue used