Specific Process Knowledge/Thermal Process/Oxidation/Breakdown voltage measurements/C3 furnace break-down voltage measurement results
Appearance
Breakdown voltage results for the C3 Anneal-Bond furnace
Dry oxidation
| Date | Oxidation recipe | Oxide thickness | Absolute break-down voltage | Relative break-down voltage
= Absolute break-down voltage/oxide thickness |
| November 2023 | DRY1100 | 488 nm |
The break-down voltage measurements have been made with help from Kitty Steenberg and Rune Sixten Grass from DTU Health Tech.