Breakdown voltage results for the C3 Anneal-Bond furnace

Dry oxidation

Date Oxidation recipe Oxide thickness Absolute break-down voltage Relative break-down voltage

= Absolute break-down voltage/oxide thickness

November 2023 DRY1100 488 nm

The break-down voltage measurements have been made with help from Kitty Steenberg and Rune Sixten Grass from DTU Health Tech.