Jump to content

LabAdviser/314/Microscopy 314-307/TEM/Tips/No-STEM

From LabAdviser
Revision as of 15:38, 22 January 2021 by Jenk (talk | contribs) (Created page with "'''Feedback to this page''': '''[mailto:labadviser@nanolab.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.nanolab.dtu.dk/index.php/LabAdviser/Microscopy_314-307/...")
(diff) ← Older revision | Latest revision (diff) | Newer revision → (diff)

Feedback to this page: click here

(content by Jens Kling, Janyary 2021)


No STEM buttons for acquisition

If case you don't see the "Search" and "Acquire" buttons in the STEM control panel, then TIA (the build in acquisition software) might not be running:

STEM control panel without TIA running


  1. Go to the task bar and find "TIA".
Task bar icon to start TIA


  1. Restart TIA.
  1. The STEM control panel should look like this now.
STEM control panel with TIA running