Revision as of 11:53, 26 January 2009 by Yg (talk | contribs) (New page: The furnace A4 phosphorus predep can be used to predeposit silicon wafers with phosphor. The silicon wafers are positioned in a quarts boat. Phosphor is predeposited in the silicon wafers.)
(diff) ← Older revision | Latest revision (diff) | Newer revision → (diff)

The furnace A4 phosphorus predep can be used to predeposit silicon wafers with phosphor. The silicon wafers are positioned in a quarts boat. Phosphor is predeposited in the silicon wafers.