Probe Station
Feedback to this page: click here
Thickness measurer
The purpose is to measure the thickness of wafers, depths of larger grooves or height of larger mesas.
During a KOH etch it can be helpful to ensure no over-etching by making a thickness measurement during the etching.
Purpose |
Thickness measurer |
|
---|---|---|
Performance |
Thickness resolution |
|
Substrates |
Batch size |
|
Substrate materials allowed |
|
The Probe station is a - EPS150Triax - Cascade for I/V measurement, ohmic measurements etc, it has 4 individually adjustable probes, but can be fitted with more. It has several source meters, multi meters and a computer attached.
It can be used from pieces up to 6" wafers
File:Probestation.jpg
Probe station: positioned in Service room CX1
The user manual, technical information and contact information can be found in LabManager: