Specific Process Knowledge/Thermal Process/A3 Phosphor Drive-in furnace
Appearance
A3 Furnace Phosphorus drive-in
A3 Furnace phosphorus drive-in is a Tempress horizontal furnace for oxidation of silicon wafers, annealing of the grown oxide, drive-in of phosphor after a pre-deposition. Phospher pre-deposition takes place in the A4 Furnace phosphorus pre-dep. A3 can also be used for drive in of phosphor which has been ion implanted.
A3 is the third furnace tube in the A-stack positioned in cleanroom 2. The A-stack together with furnace C1 are the cleanest of all our furnaces. Please be aware of which substrates are allowed to enter this furnace. Check the cross contamination chart. If you are in doubt, please ask one from the furnace team.
Process knowledge
- Phosphorus drive-in: look at the Dope with Phosphorus page
- Oxidation: look at the Oxidation page
- Annealing: look at the Annealing page
| Purpose | Drive-in of phosphor, oxidation and annealing | Oxidation:
|
|---|---|---|
| Performance | Film thickness |
|
| Process parameter range | Process Temperature |
|
| . | Process pressure |
|
| . | Gas flows |
|
| Substrates | Batch size |
|
| . | Substrate material allowed |
|