Doping your wafer
This page is about doping your wafer or making a thin film layer doped with boron, phosphor or Germane.
- PECVD - Making boron glass (BSG), phosphorus glass (PSG), boron-phosphorus glass PBSG or germanium doped glass
- Furnace LPCVD PolySilicon - Deposition of PolySi doped with B or P
- Dope with Boron - Doping Silicon wafers with boron by thermal predeposition and drive-in
- Dope with Phosphorus - Doping Silicon wafers with phosphorus by thermal predeposition and drive-in
- Ion implantation
Comparison of different doping processed
Phosphorous predep | Boron predep | PECVD doped thin film | Doped Poly Si | |
---|---|---|---|---|
Generel description | Dopants introduced by diffusion from gas-phase (POCL) | Dopants introduced by diffusion from solid source wafers | Deposition of doped thin film (oxides or nitrides) | Dopants introduced by in-situ doping of poly/amorphous Si |
Temperature1 |
|
|
|
|
Parameter 2 |
|
|
|
|
Substrate size |
|
|
|
|
Allowed materials |
|
|
|
|
1 In most cases you need a high temperature step to drive in and redistribute the dopant in the material. This is done at 800°C - 1100°C in either high temperature annealing furnaces or by rapid thermal annealing.
Ion implantation
Ion implantation cannot be done at Danchip. IBS offers ion-beam implantation as a service. See more at: http://www.ion-beam-services.com/about_us.htm