Original file (3,180 × 2,439 pixels, file size: 67 KB, MIME type: image/png)

Test of Predep with Phosphorus. Resistivity graph

File history

Click on a date/time to view the file as it appeared at that time.

Date/TimeThumbnailDimensionsUserComment
current09:41, 19 May 2014Thumbnail for version as of 09:41, 19 May 20143,180 × 2,439 (67 KB)Mdyma (talk | contribs)The old version was wrong
09:39, 19 May 2014No thumbnail3,180 × 2,439 (67 KB)Mdyma (talk | contribs)
15:01, 27 February 2013Thumbnail for version as of 15:01, 27 February 20133,180 × 2,439 (50 KB)Mdyma (talk | contribs)Test of Predep with Phosphorus. Resistivity graph