SiO2 can be etched in the Plasma Asher using CF4
Test work done January 2014 by Berit G. Herstrøm @Danchip
SiO2 can be etched in the Plasma Asher using CF4. This gives an isotropic etch.
- Images of isotropic SiO2 etch in the Plasma asher
-
Profile image - a little rotated
-
Profile image
-
Tilted profile image of lines
-
Tilted profile image of lines