- 12:47, 16 September 2025 Pevo talk contribs created page Specific Process Knowledge/Thermal Process/Oxidation/Breakdown voltage measurements/C3 furnace break-down voltage measurement results (Created page with "==Breakdown voltage results for the C3 Anneal-Bond furnace== ===Dry oxidation=== {| border="2" cellspacing="2" cellpadding="5" style="text-align: center;" |- |'''Date''' |'''Oxidation recipe''' |'''Oxide thickness''' |'''Absolute break-down voltage''' |'''Relative break-down voltage''' <i>= Absolute break-down voltage/oxide thickness<i> |- |'''November 2023''' |DRY1100 |488 nm |350x350px|thumb|left |image:...")