Main public logs
Appearance
Combined display of all available logs of LabAdviser. You can narrow down the view by selecting a log type, the username (case-sensitive), or the affected page (also case-sensitive).
- 12:42, 16 September 2025 Pevo talk contribs created page Specific Process Knowledge/Thermal Process/Oxidation/Breakdown voltage measurements/A3 furnace break-down voltage measurement results (Created page with "==Breakdown voltage results for the A3 Phosphorus Drive-in furnace== ===Dry oxidation=== {| border="2" cellspacing="2" cellpadding="5" style="text-align: center;" |- |'''Date''' |'''Oxidation recipe''' |'''Oxide thickness''' |'''Absolute break-down voltage''' |'''Relative break-down voltage''' |- |'''November 2021''' |DRY1050 |118 nm |350x350px|thumb|left |image:2021-11-09_08-27-49_Wafer_A3_DRY1050_118nm_R...")