Micro Transfer Printer
Micro transfer printing is an emerging technique to transfer diverse and non-native components from source substrate to target substrate. Micro transfer printing is best for achieving heterogeneous integration, where micro-components from different sources are picked up by polymer stamp and preciesly assembled onto different target substrate such as glass, plastic, ceramic and silicon. This method is known for increasing functinality and improving efficiency.
Micro transfer printer 100 from Xdisplay was installed in year 2022 and placed in cleanroom E-4.
Equipment info in LabManager - requires login
TextTextTextTextTextText TextText
| Purpose |
Pick and Print | |
|---|---|---|
| Material handling configuration |
Manual | |
| Stage max. travel time (X x Y mm) |
300 x 300 | |
| Source size (mm) |
upto 150 | |
| Target size (mm) |
upto 150 | |
| Alignment accuracy (single post stamp) |
<0.5um | |
| Allowed material |
All cleanroom materials
| |