Etching of aluminium can be done either by wet etch, dry etch or by sputtering with ions.
Comparison of Aluminium Etch Methods
Aluminium Etch | Developer TMAH manual | ICP metal | IBE (Ionfab300+) | |
---|---|---|---|---|
Generel description | Wet etch of Al | Wet etch/removal: TMAH Mainly used for removing Al on e-beam resist after e-beam exposure, see process flow here |
Dry plasma etch of Al | Sputtering of Al - pure physical etch. |
Etch rate range |
|
|
|
|
Etch profile |
|
|
|
|
Substrate size |
|
|
|
Smaller pieces glued to carrier wafer
|
Allowed materials | In 'Aluminium Etch' bath:
In beaker:
|
|
|
|