Etching of Aluminium
Etching of aluminium can be done either by wet etch, dry etch or by sputtering with ions.
Comparison of Aluminium Etch Methods
Al wet etch 1 | Al wet etch 2 | Developer TMAH manual | ICP metal | IBE (Ionfab300+) | |
---|---|---|---|---|---|
Generel description | Wet etch of pure Al | Wet etch of Al + 1.5% Si | Wet etch/removal: TMAH | Dry plasma etch of Al | Sputtering of Al - pure physical etch |
Etch rate range |
|
|
|
|
|
Etch profile |
|
|
|
|
|
Substrate size |
|
|
|
|
Smaller pieces glued to carrier wafer
|
Allowed materials |
|
|
|
|
|