THIS PAGE IS UNDER CONSTRUCTION
Feedback to this page: click here
Deposition of aluminium oxide
Aluminium oxide (Alumina, Al2O3 ) can be deposited by use of ALD (atomic layer deposition) or by a sputter technique in the Lesker Sputter System or the Cryofox PVD co-sputter/evaporation. During the sputter deposition oxygen is added to the chamber resulting in aluminium oxide on the sample
Comparison of the methods for deposition of Titanium Oxide
|
|
Sputter technique using IBE/IBSD Ionfab300
|
Sputter System Lesker
|
III-V Dielectric evaporator
|
ALD Picosun 200
|
| Generel description
|
- TiO2 created from a Ti sputter target. By adding oxygen during the deposition TiO2 is created.
|
- Reactive DC sputtering of Ti target in Ar/O2 (10% O2) plasma.
- RF sputtering of TiO2 target
|
- E-beam evaporation of TiO2
|
- ALD (atomic layer deposition) of TiO2
|
| Stoichiometry
|
- Can probably be varied (sputter target: Ti, O2 added during deposition)
|
|
|
- Temperature dependent - Anatase or amorphous TiO2
|
| Film Thickness
|
|
|
|
|
| Deposition rate
|
- 3.0-3.5nm/min (reactive DC sputtering)
|
- 3 - 5 nm/min (RF sputtering)
- 0.3 - 0.5nm/min
|
|
|
| Step coverage
|
|
|
|
- Very good. Covers sample everywhere (but long purge time needed for very high aspect ratio structures)
|
| Process Temperature
|
- Expected to be below 100oC
|
- Done at RT. There is a possibility to run at higher temperatures
|
- Sample temperature can be set to 20-250 oC
|
- 120oC - 150oC: Amorphous TiO2
- 300oC - 350oC: Anatase TiO2
|
| More info on TiO2
|
|
|
|
|
| Substrate size
|
- 1 50mm wafer
- 1 100mm wafer
- 1 150mm wafer
- 1 200mm wafer
- Smaller pieces can be mounted with capton tape
|
- several small samples
- several 50 mm wafers (Ø150mm carrier)
- 1x 100 mm wafers
- 1x 150 mm wafers
|
- 1x 2" wafer or
- several smaller samples
|
- 1-5 100 mm wafers
- 1-5 150 mm wafers
- Several smaller samples
|
| Allowed materials
|
- Almost any materials
- not Pb and very poisonous materials
|
- Almost any materials
- Pb and poisonous materials only after special agreement
|
|
- Silicon
- Silicon oxide, silicon nitride
- Quartz/fused silica
- Al, Al2O3
- Ti, TiO2
- Other metals (use dedicated carrier wafer)
- III-V materials (use dedicated carrier wafer)
- Polymers (depending on the melting point/deposition temperature, use carrier wafer)
|