Doping your wafer
This page is about doping your wafer or making a thin film layer doped with boron, phosphor or Germane.
- PECVD - Making boron glass (BSG), phosphorus glass (PSG), boron-phosphorus glass PBSG or germanium doped glass
- Furnace LPCVD PolySilicon - Deposition of PolySi doped with B or P
- Dope with Boron - Doping Silicon wafers with boron by thermal predeposition and drive-in
- Dope with Phosphorus - Doping Silicon wafers with phosphorus by thermal predeposition and drive-in
- Ion implantation
Comparison method 1 and method 2 for the process
Phosphor predep | Boron predep | Doped Poly Si | PECVD doped thin film | |
---|---|---|---|---|
Generel description | Dopants introduced by diffusion from gas-phase (POCL) | Dopants introduced by diffusion from solid source wafers | Dopants introduced by in-situ doping of poly/amorphous Si | Deposition of doped thin film (oxides or nitrides) |
Parameter 1 |
|
|
|
|
Parameter 2 |
|
|
|
|
Substrate size |
|
|
|
|
Allowed materials |
|
|
|
|
Ion implantation
Ion beam implantation cannot be done at Danchip. IBS offers ion-beam implantation as a service. See more at: http://www.ion-beam-services.com/about_us.htm