Jump to content

Specific Process Knowledge/Lithography/LiftOff

From LabAdviser

Lift-off Wet Bench

 
Acetone lift-off: positioned in cleanroom 3

This bench is only for wafers with metal!

Here are the main rules for lift-off bench use:

  • Place the wafers in a dedicated wafer holder.
  • Put the holder in the acetone and start the ultrasound. The strip off time is depending of resist thickness.
  • Rinse your wafers for 4-5 min. in running water after stripping.

Find more info about the lift-off process here: Specific Process Knowledge/Photolithography/AZ5214E standard resist - reverse process