Jump to content

Specific Process Knowledge/Thermal Process/Oxidation/Breakdown voltage measurements/C3 furnace break-down voltage measurement results

From LabAdviser
Revision as of 12:53, 16 September 2025 by Pevo (talk | contribs) (Breakdown voltage results for the C3 Anneal-Bond furnace)
(diff) ← Older revision | Latest revision (diff) | Newer revision → (diff)

Breakdown voltage results for the C3 Anneal-Bond furnace

Dry oxidation

Date Oxidation recipe Oxide thickness Absolute break-down voltage Relative break-down voltage

= Absolute break-down voltage/oxide thickness

November 2023 DRY1100 488 nm

The break-down voltage measurements have been made with help from Kitty Steenberg and Rune Sixten Grass from DTU Health Tech.