Specific Process Knowledge/Characterization/Optical microscope
Feedback to this page: click here
This page is written by DTU Nanolab internal
Nikon SMZ 1000 | Noco IR | Leica INM 100 | Nikon Eclipse L200 #2 | Zeiss Jenatech | Nikon Eclipse L200 #1 | Nikon Eclipse L200N #3 | Nikon Eclipse L200N #4 | Nikon ME 600 | Leica S8 APO | Zeiss Axiotron | |
---|---|---|---|---|---|---|---|---|---|---|---|
![]() |
![]() ![]() |
![]() |
![]() ![]() |
![]() ![]() |
![]() ![]() |
![]() |
![]() |
![]() ![]() |
![]() |
![]() ![]() | |
Location | 346-901 | 346-901 | 346-901 | cleanroom F3 | cleanroom A1 | cleanroom D3 | cleanroom E4 | cleanroom E5 | cleanroom F1 | cleanroom Cx1 | cleanroom D3 |
Responsible group | Wet chemistry | Wet chemistry | Wet chemistry | Lithography | Lithography | Lithography | Lithography | Lithography | Lithography | Lithography | Lithography |
Objectives | Zoom 0.8x - 8x |
|
|
|
|
|
|
|
|
Zoom 1x - 8x |
|
Ocular | 10x | 10x | 10x | 10x | 10x | 10x | 10x | 10x | 10x | 10x | 10x |
Special features | Stereoscopic microscope | IR imaging |
|
Stereoscopic microscope | |||||||
Contrast mechanisms |
|
|
|
|
|
|
|
|
|
|
|
Illumination modes |
|
|
|
|
|
|
|
|
|
|
|
Camera | None | IR camera | DS-Fi2 | DS-Fi1 | None | DS-Fi1 |
|
|
DS-Fi2 | None | Infinity X |
Analysis software | None | None | NIS-D | NIS-D | None | NIS-BR | NIS-D | NIS-D | NIS-D | None | DeltaPix |
There are also two optical microscopes in building 451, a stereo microscope and a transmission microscope, that were both previously located in Packlab. Please ask staff / the BioMic group for details.