Specific Process Knowledge/Etch/DRIE-Pegasus/Pegasus-2
Appearance
Feedback to this page: click here
This system is a research tool and not available to the users
If you want to get access to the tool, then talk to professor Henry Jansen
Current setup and rules on Pegasus 2
Click here to access older configurations.
The current configuration is
| Item | The currently applied modification | Comments |
|---|---|---|
| Available gasses and gas chemistry | * C4<\sub>F8<\sub> (H2 currently fitted but closed) : 0 sccm
|
OnlySF6 and O2 are used for Si, PR, and Cr etch. The rest is only make-up |
Access to Pegasus 2 configuration templates
Pegasus 2 configuration table version 1
- Table header: Template:Peg2configheader1
- Table content: Template:Peg2configcontent1