The furnace A4 phosphorus predep(N-predep) can be used to predeposit silicon wafers with phosphor. The silicon wafers are positioned in a quarts boat. Phosphor is predeposited in the silicon wafers.
The furnace A4 phosphorus predep(N-predep) can be used to predeposit silicon wafers with phosphor. The silicon wafers are positioned in a quarts boat. Phosphor is predeposited in the silicon wafers.


'''In preparation'''
'''
== In preparation ==
'''

Revision as of 14:27, 26 November 2012

The furnace A4 phosphorus predep(N-predep) can be used to predeposit silicon wafers with phosphor. The silicon wafers are positioned in a quarts boat. Phosphor is predeposited in the silicon wafers.

In preparation