LabAdviser/314/Microscopy 314-307/TEM: Difference between revisions
mNo edit summary |
|||
| Line 24: | Line 24: | ||
| align="center" width="200px" | '''Titan ETEM''' [[image:Microscopy-icon_TEM.png|180px|frameless |border |link=LabAdviser/314/Microscopy_314-307/TEM/ETEM|Titan ETEM ]] | | align="center" width="200px" | '''Titan ETEM''' [[image:Microscopy-icon_TEM.png|180px|frameless |border |link=LabAdviser/314/Microscopy_314-307/TEM/ETEM|Titan ETEM ]] | ||
| align="center" width="200px" | '''Spectra Ultra''' [[image:Microscopy-icon_TEM.png|180px|frameless |border |link=LabAdviser/314/Microscopy_314-307/TEM/Spectra Ultra|Spectra Ultra]] | | align="center" width="200px" | '''Spectra Ultra''' [[image:Microscopy-icon_TEM.png|180px|frameless |border |link=LabAdviser/314/Microscopy_314-307/TEM/Spectra Ultra|Spectra Ultra]] | ||
| align="center" width="200px" | '''Talos''' [[image:Microscopy-icon_TEM.png|180px|frameless |border |link=LabAdviser/314/Microscopy_314-307/TEM/Talos|Talos]] | |||
|} | |} | ||
Revision as of 13:21, 23 September 2026
The content on this page, including all images and pictures, was created by DTU Nanolab staff, unless otherwise stated.
Feedback to this page: click here
TEM
Transmission Electron Microscopy (TEM) is a technique, where accelerated electrons penetrate a thin sample and are collected on a detector. Dependenging on the type of detector, different signals and sample characteristics can be acquired. The electron beam is steered by electromagnetic lenses.
We have five TEMs available at DTU Nanolab. Click on the instrument to find more information about the equipment and available techniques:
| Tecnai T12 Biotwin |
Tecnai T20 |
Titan ATEM |
| Titan ETEM |
Spectra Ultra |
Talos |
Comparison between TEMs at DTU Nanolab - building 314/307
| Microscope | |||||
|---|---|---|---|---|---|
| Purpose |
|
|
|
| |
| Resolution | TEM mode |
>3.5 Å |
1.44 Å |
1.02 Å |
0.9 Å |
| STEM mode |
no STEM |
about 10 Å |
0.8 Å |
1.36 Å | |
| Spectroscopy | EDX |
Oxford X-Max 80T/AZtec |
Oxford X-Max 80T/AZtec |
Oxford X-Max 100TLE/AZtec |
Oxford X-Max 80T/AZtec |
| EELS |
no EELS |
Gatan 863 Tridiem GIF |
Gatan 865 Tridiem GIF |
Gatan 866 Tridiem GIF | |