Specific Process Knowledge/Lithography/UVExposure/aligner MLA2: Difference between revisions
| Line 20: | Line 20: | ||
'''Features''' | '''Features''' | ||
*Optical Autofocus | *Optical Autofocus (enables chips down to 3 x 3 mm) | ||
*Pneumatic Autofocus | *Pneumatic Autofocus | ||
*Top side Alignment | *Top side Alignment | ||
*Back side Alignment | *Back side Alignment | ||
*Gray Scale Exposure | *Gray Scale Exposure (no alignment) | ||
*Advanced Field Alignment Mode for alignment to individual chips/devices on the substrate | *Advanced Field Alignment Mode for alignment to individual chips/devices on the substrate | ||
*<del>High Aspect Ratio Mode for exposure of thick resists</del> (available but not correctly adjusted) | *<del>High Aspect Ratio Mode for exposure of thick resists</del> (available but not correctly adjusted) | ||
Latest revision as of 11:04, 3 September 2026
Aligner: Maskless 02

Tool description
The MLA2 is a UV exposure tool, which can be used for direct writing of digital mask designs, on photosensitive resists on chips, 50 mm, 100 mm, 150 mm and 200 mm substrates.
| Product: | Heidelberg Instruments MLA150 WM I Maskless Aligner |
|---|---|
| Year of purchase: | 2018 |
| Tool modification: | Modified from WM1 to WM2 in 2023 |
| Location: | Cleanroom E-5 |
Features
- Optical Autofocus (enables chips down to 3 x 3 mm)
- Pneumatic Autofocus
- Top side Alignment
- Back side Alignment
- Gray Scale Exposure (no alignment)
- Advanced Field Alignment Mode for alignment to individual chips/devices on the substrate
High Aspect Ratio Mode for exposure of thick resists(available but not correctly adjusted)- 200 x 200 mm exposure field
User manual
The user manual and contact information can be found in LabManager - requires login
Tool training
Training on the tool requires users to complete the lithography TPT followed by the online tool training and a hands-on authorization training.
| Purpose | Alignment and UV exposure |
|---|---|
| Exposure modes | Projection |
| Exposure light/filters | 375 nm (laser diode array) |
| Dynamic focusing method |
|
| Minimum resolution | ~1 µm |
| Design file formats |
|
| Alignment modes |
|
| Substrate size |
|
| Allowed materials |
|
| Substrate batch | 1 |
Process information
Exposure dose
Information on UV exposure dose
Alignment mark design and locations
Alignment mark design and locations.
Quality Control (QC)
The purpose of the QC process is to check the optical performance and alignment accuracy of the maskless aligners. The optical performance is checked by making a dose/defocus test. The alignment accuracy is checked by making a global alignment test for both topside alignment and back side alignment.
Dose/defoc limit:
Deviations in the optical performance are not easily corrected, and is likely due to contaminated or damaged writehead. If either the dose or defoc changes, the tool is investigated for writehead contamination and/or damage.
Alignment accuracy accept limit:
Must be within machine specifications, and should be adjusted if necessary. The top side alignment accuracy for MLA2 is ±0.5 µm. The backside alignment accuracy for MLA2 is ±1 µm.
Documentation:
- The QC procedure for Aligner: MLA2 - requires login
- The newest QC data for Aligner: MLA2 - requires login