Specific Process Knowledge/Lithography/Strip/plasmaAsher05: Difference between revisions
Appearance
| Line 32: | Line 32: | ||
==Process development sections== | ==Process development sections== | ||
*[[Specific Process Knowledge/Lithography/Strip/plasmaAsher04_processDevelopment| | *[[Specific Process Knowledge/Lithography/Strip/plasmaAsher04_processDevelopment|Stripping with plasma asher 04 and plasma asher 05]] | ||
*[[Specific Process Knowledge/Etch/Etching of Silicon Oxide/SiO2 etch using Plasma Asher |SiO<sub>2</sub> etch using Plasma Asher 1]] | *[[Specific Process Knowledge/Etch/Etching of Silicon Oxide/SiO2 etch using Plasma Asher |SiO<sub>2</sub> etch using Plasma Asher 1]] | ||
*[[Specific Process Knowledge/Lithography/Descum/plasmaAsher05|Descum using plasma asher 5]] | *[[Specific Process Knowledge/Lithography/Descum/plasmaAsher05|Descum using plasma asher 5]] | ||
<br clear="all" /> | <br clear="all" /> | ||
Revision as of 09:08, 25 June 2026
Plasma Asher 5

Product name: PVA Tepla Gigabatch 380M
Year of purchase: 2024
The Plasma Asher 5 can be used for the following processes:
- Photoresist stripping
- Descumming
- Surface cleaning
- Removal of organic passivation layers and masks
Furthermore plasma processing using CF4 in plasma asher 5 can be used for:
- Etching of glass and ceramic
- Etching of SiO2, Si3N4, Si
- Removal of polyimide layers
Plasma asher 5 can be used for almost every material, but if you have any doubt if your materials are compatible/allowed in plasma asher 5, feel free to ask the lithography group at Nanolab.
The user manual, risk assessment, and contact information can be found in LabManager - requires login
Process Information
Typical stripping parameters
Tested with 1.5 µm AZ 5214E on 100 mm silicon substrate.
- O2: 100 sccm
- N2: 100 sccm
- Pressure (DSC): 1.3 mbar
- Power: 1000 W
- Time (single wafer): 20-30 minutes
- Time (full boat): 90 minutes
Process development sections
- Stripping with plasma asher 04 and plasma asher 05
- SiO2 etch using Plasma Asher 1
- Descum using plasma asher 5