Jump to content

Specific Process Knowledge/Lithography/Development/DUV developer: Difference between revisions

Jehem (talk | contribs)
Jehem (talk | contribs)
Line 87: Line 87:
|style="background:WhiteSmoke; color:black"|
|style="background:WhiteSmoke; color:black"|
*AZ 726 MIF (TMAH): 500 ml/min
*AZ 726 MIF (TMAH): 500 ml/min
*Process DI water: 400 ml/min
*Process DI water: 350 ml/min (with BSR+CR active)
*Backside rinse DI water: 60 ml/min
*Backside rinse DI water: 45 ml/min (with TSR+CR active)
*Process Nitrogen: 50 l/min
*Process Nitrogen: 50 l/min
|-
|-
|}
|}
<br clear="all" />
<br clear="all" />