Specific Process Knowledge/Lithography/Development/UV developer: Difference between revisions
Appearance
Tag: Manual revert |
Tag: Manual revert |
||
| Line 82: | Line 82: | ||
|style="background:WhiteSmoke; color:black"| | |style="background:WhiteSmoke; color:black"| | ||
*AZ 726 MIF (TMAH): 230 ml/min | *AZ 726 MIF (TMAH): 230 ml/min | ||
*Process DI water: 400 ml/min (with BSR+CR) | *Process DI water: 400 ml/min (with BSR+CR active) | ||
*Backside rinse DI water: 55 ml/min (with TSR+CR) | *Backside rinse DI water: 55 ml/min (with TSR+CR active) | ||
*Process Nitrogen: 50 l/min | *Process Nitrogen: 50 l/min | ||
|- | |- | ||
|} | |} | ||
<br clear="all" /> | <br clear="all" /> | ||