*For Top Side Alignment (TSA) alignment marks should be located 35-80 mm in left and right in horizontal location (X) from mask center and between -20 and +20 mm in vertical location (Y)
*For Top Side Alignment (TSA) alignment marks should be located 35-80 mm in left and right in horizontal location (X) from mask center and between -20 and +20 mm in vertical location (Y)
*For Top Side Alignment (BSA) alignment marks should be located 15-45 mm in left and right in horizontal location (X) from mask center and between -20 and +20 mm in vertical location (Y)
*For Back Side Alignment (BSA) alignment marks should be located 15-45 mm in left and right in horizontal location (X) from mask center and between -20 and +20 mm in vertical location (Y)