Created page with "==Breakdown voltage results for the C1 Anneal-Oxide furnace== ===Dry oxidation=== {| border="2" cellspacing="2" cellpadding="5" style="text-align: center;" |- |'''Date''' |'''Oxidation recipe''' |'''Oxide thickness''' |'''Absolute break-down voltage''' |'''Relative break-down voltage''' <i>= Absolute break-down voltage/oxide thickness<i> |- |'''October 2023''' |DRY1100 |510 nm |350x350px|thumb|left..." |
|||
| Line 19: | Line 19: | ||
|- | |- | ||
|} | |} | ||
<i>The break-down voltage measurements have been made with help from Kitty Steenberg and Rune Sixten Grass from DTU Health Tech.<i> | |||
Latest revision as of 12:53, 16 September 2025
Breakdown voltage results for the C1 Anneal-Oxide furnace
Dry oxidation
| Date | Oxidation recipe | Oxide thickness | Absolute break-down voltage | Relative break-down voltage
= Absolute break-down voltage/oxide thickness |
| October 2023 | DRY1100 | 510 nm |
The break-down voltage measurements have been made with help from Kitty Steenberg and Rune Sixten Grass from DTU Health Tech.