Jump to content

Specific Process Knowledge/Thermal Process/D4 III-V Oven: Difference between revisions

From LabAdviser
Mmat (talk | contribs)
mNo edit summary
Mmat (talk | contribs)
 
Line 24: Line 24:


'''[http://www.labmanager.danchip.dtu.dk/function.php?module=Machine&view=view&mach=187 III-V Oven (D4)]'''
'''[http://www.labmanager.danchip.dtu.dk/function.php?module=Machine&view=view&mach=187 III-V Oven (D4)]'''
==Process knowledge==
*[[Specific_Process_Knowledge/Thermal_Process/Oxidation/Oxidation_on_III-V_furnace_(D4)|Standard wet oxidation recipe on the III-V furnace]]


==Overview of the performance of the III-V Oven and some process related parameters==
==Overview of the performance of the III-V Oven and some process related parameters==

Latest revision as of 16:18, 3 June 2025

The content on this page, including all images and pictures, was created by DTU Nanolab staff, unless otherwise stated.

Feedback to this page: click here

The D4 III-V Oven has been decomission in August 2019.


III-V Oven (D4)

III-V Oven (D4). Positioned in cleanroom area F-3/ Photo: DTU Nanolab internal.

The III-V Oven (D4) is used for wet thermal oxidation of III-V devices, for instance for lateral oxidation of thin AlGaAs layers to defined apertures in light-limiting diodes.

The furnace is an old Tempress horizontal furnace. The quartz boat is loaded manually into the furnace by use of a push rod. The furnace is cooled down to room temperature when it is not being used.

Before use, devices have to be cleaned. A short BHF dip can be used to remove any native oxide which can be difficult to penetrate by a wet thermal oxidation.

Please check the cross contamination information in LabManager before you use the furnace.

The user manual and contact information can be found in LabManager:

III-V Oven (D4)

Overview of the performance of the III-V Oven and some process related parameters

Purpose
  • Wet oxidation of III-V dvices
Performance Lateral oxidation rate
  • Very sample dependent
Process parameter range Process temperature
  • 420 oC
Process pressure
  • 1 atm
Gasses on the system
  • N2 (bobler)
  • N2
Substrates Batch size
  • Several smaller samples (placed vertically on a quartz plate)
Substrate materials allowed
  • III-V devices
  • Silicon