== Dektak 3ST ==
info moved to
 
https://labadviser.nanolab.dtu.dk//index.php?title=Specific_Process_Knowledge/Characterization/Dektak_3ST#Dektak_3ST
 
[[image:III-V profiler.JPG|300x300px|right|thumb|The profiler placed in 346-904 (Dektak 3ST).]]
 
The Dektak 3ST is intended for profile measurements on samples outside the cleanroom. It is located in the basement, building 346, room 904.
 
 
'''The user manual, technical information and contact information can be found in LabManager:'''
 
[http://labmanager.danchip.dtu.dk/function.php?module=Machine&view=view&mach=184 Dektak 3ST (Dektak) in LabManager]
 
The computer connected to the Dektak 3ST is pretty old and runs Windows 98 SE. It is not connected to the network but traces can be saved on either USB memory stick or floppy disk. The USB driver is an old universal driver and has been shown to work with small size USB sticks. However it did not work with an 8GB Kingston stick.
 
===Equipment performance and process related parameters===
{| border="2" cellspacing="0" cellpadding="10"
|-
!style="background:silver; color:black" align="left" rowspan="4" valign="top" |Performance
|style="background:LightGrey; color:black"|Vertical Range
|style="background:WhiteSmoke; color:black"|
*65 kÅ, 655 kÅ, 1310 kÅ
|-
|style="background:LightGrey; color:black"|Scan length range
|style="background:WhiteSmoke; color:black"|
*50-50000 µm
|-
|style="background:LightGrey; color:black"|Stylus track force
|style="background:WhiteSmoke; color:black"|
*Recommended: 3-10 mg, depending on the softness of the surface
|-
|style="background:LightGrey; color:black"|Scan speed ranges
|style="background:WhiteSmoke; color:black"|
*High speed: 3s for 50µm to 50000µm
*Medium speed: 12s for 50µm to 10000µm
*Low speed: 50s
|-
!style="background:silver; color:black" align="left" rowspan="1" valign="top" |Materials
|style="background:LightGrey; color:black"|Allowed substrate materials
|style="background:WhiteSmoke; color:black"|
*III-V
* Silicon
* polymer
|}


== Stylus Profiler: Dektak150 ==