There are different file formats available and not all equipment can handle each of them. | There are different file formats available and not all equipment can handle each of them. | ||
* For '''UV-lithography''', you create a layout file with your design. The file format should preferably be CIF or GDS, though DXF, or GERBER is acceptable too. The electronic mask layout can be used directly in one of our [[Specific Process Knowledge/Lithography/UVExposure|Mask Less Aligners (MLAs)]] or you can have a physical mask produced based on the layout file for our [[Specific_Process_Knowledge/Lithography/UVExposure#Aligner:_MA6-2|Mask Aligner]]. For more details see below [[Specific_Process_Knowledge/Pattern_Design#Mask_Ordering_and_Fabrication|Mask Fabrication for UV-lithography]]. | * For '''UV-lithography''', you create a layout file with your design. The file format should preferably be CIF or GDS, though DXF, or GERBER is acceptable too. The electronic mask layout can be used directly in one of our [[Specific Process Knowledge/Lithography/UVExposure|Mask Less Aligners (MLAs)]] or you can have a physical mask produced based on the layout file for our [[Specific_Process_Knowledge/Lithography/UVExposure#Aligner:_MA6-2|Mask Aligner]]. For more details see below [[Specific_Process_Knowledge/Pattern_Design#Mask_Ordering_and_Fabrication|Mask Fabrication for UV-lithography]]. | ||
* For '''DUV-lithography''', a physical mask, called "reticles", is required. The file format must be GDS. For more details concerning the design of reticles see [[Specific_Process_Knowledge/Lithography/DUVStepperLithography | * For '''DUV-lithography''', a physical mask, called "reticles", is required. The file format must be GDS. For more details concerning the design of reticles see [[Specific_Process_Knowledge/Lithography/DUVStepperLithography/Reticle_Design|Design of Reticles]]. | ||
* For '''E-beam lithography''', you need to prepare a set of files (GDS, V30, sdf, jdf and mgn files). For more details, please see [[Specific_Process_Knowledge/Lithography/EBeamLithography/FilePreparation#FilePreparation|File preparation]]. For details about how to make aligned E-beam patterns, please have at look at [[Specific_Process_Knowledge/Lithography/EBeamLithography/JBX9500Manual#Design_of_global_marks_and_chip_marks|Design of global marks and chip marks]] | * For '''E-beam lithography''', you need to prepare a set of files (GDS, V30, sdf, jdf and mgn files). For more details, please see [[Specific_Process_Knowledge/Lithography/EBeamLithography/FilePreparation#FilePreparation|File preparation]]. For details about how to make aligned E-beam patterns, please have at look at [[Specific_Process_Knowledge/Lithography/EBeamLithography/JBX9500Manual#Design_of_global_marks_and_chip_marks|Design of global marks and chip marks]] | ||
* For '''Laser Cutting''' using our [Specific Process Knowledge/Back-end processing/Laser Micromachining Tool|Laser Micromachining Tool], the layout file must be saved as DXF file. | * For '''Laser Cutting''' using our [Specific Process Knowledge/Back-end processing/Laser Micromachining Tool|Laser Micromachining Tool], the layout file must be saved as DXF file. | ||
<br> | <br> | ||
<br> | <br> | ||
== Mask Design for UV-lithography == | == Mask Design for UV-lithography == | ||
Here you can find tips and tricks for mask designing. | Here you can find tips and tricks for mask designing. | ||