The content on this page, including all images and pictures, was created by DTU Nanolab staff, unless otherwise stated.
Feedback to this page: click here
Plasma Asher 1
This tool has been decommissioned 2024-12-02.
Information about decommissioned tool
Plasma Asher 2
Jitka Urbánková & Jesper Hanberg, December 2019

This tool has been decomissioned 2024-12-02.
The user manual(s), quality control procedure(s) and results and contact information can be found in LabManager - requires login
Descum of AZ Mir 701 resist on 100mm silicon wafer. Five wafers were placed vertically in chamber.
recipe 1:
- O2 flow: 100 ml/min
- N2 flow: 100 ml/min
- Power: 150 W
|

recipe 2:
- O2 flow: 500 ml/min
- N2 flow: 0 ml/min
- Power: 200 W
|
A linear time dependence was observed after etching 7 minutes or more (recipe 2).
Plasma Asher 3: Descum
The user manual(s), quality control procedure(s) and results and contact information can be found in LabManager - requires login
Plasma Asher 3 is specifically used for controlled descum process after lithography. Please note that you only can process a single 100 mm wafer, or one small sample, at a time. The plasma asher is equipped with 2 gaslines: oxygen and nitrogen, but all standard processes use only oxygen (as recommended by Diener).
Ashing of AZ MiR701 resist:
You can use two different descum process developments: you can either change power settings or processing chamber pressure.
Testing different power settings:

Recipe settings:
- O2 flow: 5 sccm
- N2 flow: 0
- Pressure: 0.2 mbar
- Power: Varied
Experiment parameters:
|
Testing different pressure settings:

Recipe settings:
- O2 flow: varied
- N2 flow: 0
- Pressure: varied
- Power: V100% (100 W)
Experiment parameters:
|
Ashing of AZ5214E resist:

Recipe settings:
- O2 flow: varied
- N2 flow: 0
- Pressure: varied
- Power: V100% (100 W)
Experiment parameters:
|