Specific Process Knowledge/Back-end processing/Micro transfer printer: Difference between revisions
| Line 10: | Line 10: | ||
[[File:MTP.tif|thumb]] | [[File:MTP.tif|thumb]] | ||
=Micro Transfer Printer= | =Micro Transfer Printer= | ||
[[ | |||
[[Image:MTP image.jpg|1000px|frameless|right|]] | |||
Micro transfer printing is an emerging technique to transfer diverse and non-native components from source substrate to target substrate. Micro transfer printing is best for achieving heterogeneous integration, where micro-components from different sources are picked up by polymer stamp and precisely assembled onto different target substrate such as glass, plastic, ceramic and silicon. This method is known for increasing functionality and improving efficiency. | Micro transfer printing is an emerging technique to transfer diverse and non-native components from source substrate to target substrate. Micro transfer printing is best for achieving heterogeneous integration, where micro-components from different sources are picked up by polymer stamp and precisely assembled onto different target substrate such as glass, plastic, ceramic and silicon. This method is known for increasing functionality and improving efficiency. | ||
Revision as of 11:26, 8 September 2023
The content on this page, including all images and pictures, was created by DTU Nanolab staff, unless otherwise stated.
Feedback to this page: click here
Micro Transfer Printer

Micro transfer printing is an emerging technique to transfer diverse and non-native components from source substrate to target substrate. Micro transfer printing is best for achieving heterogeneous integration, where micro-components from different sources are picked up by polymer stamp and precisely assembled onto different target substrate such as glass, plastic, ceramic and silicon. This method is known for increasing functionality and improving efficiency.
Micro transfer printer 100 from Xdisplay was installed in year 2022 and placed in cleanroom F-4.
Equipment info in Lab Manager - requires login
| Purpose |
Pick and Print | |
|---|---|---|
| Material handling configuration |
Manual | |
| Stage max. travel time (X x Y mm) |
300 x 300 | |
| Source size (mm) |
upto 150 | |
| Target size (mm) |
upto 150 | |
| Alignment accuracy (single post stamp) |
<0.5um | |
| Allowed material |
All cleanroom materials
| |