DRIE-Pegasus 4 is dedicated Silicon oxide and Silicon nitride etching. It is originally designed for silicon etching but gas mass flow controllers has been changed to optimize silicon oxide and silicon nitride etching. The system is setup for 6" wafers. Sampler samples has to be bonded to a 6" carrier to be etched in the system. | |||
[[Image:Peg3and4 front 2.JPG |frame|right|x300px|The DRIE-Pegasus3 and DRIE-Pegasus4 operator station and cassette loading stations, {{photo1}}]] | [[Image:Peg3and4 front 2.JPG |frame|right|x300px|The DRIE-Pegasus3 and DRIE-Pegasus4 operator station and cassette loading stations, {{photo1}}]] | ||
Revision as of 11:37, 22 August 2023
Feedback to this page:
click here
Template:CC1
Pegasus 4 - 150mm silicon oxide and silicon nitride etching
DRIE-Pegasus 4 is dedicated Silicon oxide and Silicon nitride etching. It is originally designed for silicon etching but gas mass flow controllers has been changed to optimize silicon oxide and silicon nitride etching. The system is setup for 6" wafers. Sampler samples has to be bonded to a 6" carrier to be etched in the system.
The user manual and contact information can be found in LabManager:
DRIE Pegasus 4 in LabManager - requires login
Process information
Standard recipes
- Barc Etch
- SiO2 Etch
- Nitride etch with SiO2 etch recipes
- Slow etch of silicon nitride and silicon oxide
Wafer bonding